Super Systems Inc., Cincinnati, Ohio, reports that Callies Precision Engine Components has installed an SSI automated system with the ability to achieve tight nitriding process control using an easy-to-use recipe system that maintains tight tolerances on temperature, gas flow, and nitriding potential.