Researchers from ETH Zurich have explored a new passive dehumidification approach for indoor spaces, where high humidity is absorbed by walls and ceilings and temporarily stored in a hygroscopic material. This method, which releases moisture when the room is ventilated, offers an energy-efficient alternative to mechanical dehumidification systems commonly used in high-traffic areas like offices, museums, and government buildings. According to Professor Guillaume Habert, this solution is ideal for spaces where existing ventilation systems are insufficient.
Habert and his research team followed the principle of the circular economy in their search for a suitable hygroscopic material. The starting point is finely ground waste from marble quarries. A binder is needed to turn this powder into moisture-binding wall and ceiling components. This task is performed by a geopolymer, a class of materials consisting of metakaolin (known from porcelain production) and an alkaline solution (potassium silicate and water). The alkaline solution activates the metakaolin and provides a geopolymer binder that binds the marble powder to form a solid building material. The geopolymer binder is comparable to cement but emits less CO2 during its production.
In the ETH project, the scientists succeeded in producing a prototype of a wall and ceiling component measuring 20 × 20 cm and 4 cm thick. Production was carried out using 3D printing in a group led by Benjamin Dillenburger, Professor for Digital Building Technologies. In this process, the marble powder is applied in layers and glued by the geopolymer binder (binder jet printing technology). “This process enables the efficient production of components in a wide variety of shapes,” says Benjamin Dillenburger.
Combining geopolymer and 3D printing to produce a moisture reservoir is an innovative approach to sustainable construction. Building physicist Magda Posani led the study of the material’s hygroscopic properties at ETH Zurich before recently taking on a professorship at Aalto University in Espoo, Finland. The project is based on the doctoral theses of materials scientist Vera Voney, supervised by Senior Research Associate Coralie Brumaud and architect Pietro Odaglia, who developed the material and the 3D printing machine at ETH.
“We were able to demonstrate with numerical simulations that the building components can significantly reduce humidity in heavily used indoor spaces,” says Posani, summarising the main result of the research project. For the simulation, it was assumed that the walls and ceiling of a reading room used by 15 people in a public library in Oporto, Portugal had been completely lined with hygroscopic components. Magda Posani calculated how often and to what extent the humidity exceeded the comfort zone, i.e. 40 to 60 percent relative humidity in this virtual reading room over the course of a year. From this, she calculated a discomfort index, a figure that expresses the loss of comfort caused by excessively high or low humidity. If the reading room were fitted with the moisture-binding components, the discomfort index could be reduced by 75 percent compared to a conventional painted wall. If components were used that were 5 cm thick instead of just 4 cm, the discomfort index fell by as much as 85 percent.
The hygroscopic wall and ceiling components are climate-friendly, i.e. they cause significantly lower greenhouse gas emissions over a 30-year life cycle than a ventilation system that dehumidifies air quality to the same extent. In the simulation calculations, the wall and ceiling components were also compared with a clay plaster that has been used since time immemorial and also passively regulates the air humidity in indoor spaces. This old technique proved to be even more climate-friendly than the hygroscopic components. However, the plaster has a lower storage capacity for water vapour.
The research at ETH has shown that the combination of geopolymer and 3D printing can be used to produce wall and ceiling components for efficient moisture buffering. After this proof of concept, the technology is, in principle, ready to be further developed and scaled for industrial manufacture. At the same time, research continues. In a project with Turin Polytechnic and Aalto University, ETH Zurich is working to produce wall and ceiling components with even lower greenhouse gas emissions. Because one thing is clear: if Switzerland wants to achieve its net zero target by 2050, it needs buildings that cause as little greenhouse gas emissions as possible during construction and use.
For more information: Nature Communications