ASM Handbook, Volume 5A: Thermal Spray Technology


Co-published by the Thermal Spray Society and ASM International, ASM Handbook, Volume 5A: Thermal Spray Technology replaces the Handbook of Thermal Spray Technology (2004) and provides a comprehensive introduction to modern thermal spray processes—including plasma spray, HVOF, and detonation gun deposition. The volume covers coating principles, properties, performance, testing, and applications across industries such as aerospace, energy, automotive, electronics, and biomedical. It highlights advances in equipment and diagnostics that have transformed thermal spray from an art to a science, and explores emerging opportunities in environmental and thermal barrier coatings for next-generation materials and high-temperature applications.

 

TSS Members receive online access to ASM Handbook, Volume 5A: Thermal Spray Technology as part of the member benefit package. 

Please sign in to view.