Twisting crystal sheets creates tunable grids of atomic defects

Researchers at the Technical University of Denmark (DTU) have fabricated two ultrathin crystal sheets that, when stacked and rotated relative to each other, create a square lattice of defects at their interface. These defects change how electrical charges are arranged, and by bonding and twisting the 10-nanometer-thick sheets, tiny electrical patterns emerge at the interface. These controllable arrangements could eventually prove useful in the electronics industry, although using them in a working device will require further research.

The study, published in Nature, shows why strong bonding between the sheets matters for understanding their behavior.

“We have spent years learning how to make high-quality sheets, put them together in the right position, bond them and twist them. Once you can do all of that, you can start looking at what happens where these two sheets meet,” says Professor Nini Pryds of DTU. “So, the bonding is essential to understanding what happens between the layers.”

The starting point is a familiar pattern. Lay two mesh screens crosswise and rotate one slightly, and a larger repeating pattern will appear. This is a moiré pattern, and the same geometry appears when the regular atomic structures of two crystal sheets overlap at an angle.

The researchers used sheets of strontium titanate (SrTiO3) – a hard, chemically stable material often used as a model oxide in electronics. Strong bonding during the twisting allowed the atoms at the interfaces between the sheets to adopt arrangements that fit together. The remaining mismatch gathered along narrow lines of distorted crystal, known as dislocations, forming a square grid.

Modeling showed that distortions around the grid could slightly separate positive and negative charges. This separation, called polarization, formed swirling patterns. Since controlling polarization is relevant to memory and energy storage, there is a possibility that future devices could be designed based on these patterns.

“Changing the twist angle changes the spacing between the dislocations. So now, we have a way to control how small the structure becomes,” says joint first author William Sandholt. “These dislocations could be used for memory applications, for example, and the grid could be tuned through the twist angle.”

The first microscope images appeared to show an ordinary moiré pattern and offered no clear view of the grid predicted by the simulations. The team modeled how the electron beam would pass through the material and cut samples in different directions to examine the buried structure in cross-section.

“The electron beam goes through about ten nanometers of material, reaches the interface, and then goes through another ten nanometers. So, the image is influenced by the material on both sides of what we want to see,” explains John Mangeri, a postdoc at DTU and joint first author of the study. “Right where the sheets met, we could see the repeating pattern, and it agreed almost perfectly with the theory. That was amazing.”

Electron microscopy by collaborators at the University of Antwerp in Belgium and the SuperSTEM Laboratory in the UK was central to identifying and characterizing the grid. Further microscopy, interpreted alongside the simulations, supported the link between the rearranged atoms and the electrical patterns.

 

Image – Two ultrathin crystal layers, shown as blue and red atoms, are rotated relative to each other. When the layers bond strongly, their atoms rearrange into a square grid of defects in the crystal structure, highlighted here by golden lines. The spacing between the lines can be controlled by changing the twist angle between the layers. Courtesy of: John Mangeri.

 

For more information:
Technical University of Denmark
https://www.dtu.dk/english