Researchers led by the University of Rochester’s Anne S. Meyer developed a lower-cost method for creating 3D-printed living materials using a standard plastic 3D printer. These materials can contain bacteria capable of applications such as cleaning contaminated water or breaking down plastic waste, offering an alternative to specialized bioprinters that can cost more than $100,000.
To solve this, a team of researchers led by the University of Rochester’s Anne S. Meyer has developed a low-cost solution using a standard plastic 3D printer.
“We aim to create DIY bioprinters using inexpensive, easily obtainable parts, so that they are affordable and easy for other scientists to make in their own labs as well,” says Meyer, a professor in the Department of Biology.
In a recent study published in , Meyer and colleagues from URochester and Cornell University modified a regular plastic 3D printer by removing the plastic filament extruder and replacing it with a syringe pump that squeezes out bio-ink—a specialized formula that mixes living cells with a polymer solution. Once printed, the bio-ink hardens into a gel.
“Our syringe can also perform both extrusion and retraction, preventing oozing at the edges of printed structures,” says Meyer. “This new setup allows for printing of crisp shapes with well-defined edges.”
In the true spirit of DIY, Meyer’s lab constructed the customized bioprinter at a cost of $450. All the parts are easily available, adds Meyer, allowing other labs to build their own version of the printer and syringe pump.
While previous DIY 3D bioprinters were limited to printing structures of less than 20 layers, “our upgraded printer can create living structures that are significantly taller and more complex than was previously possible, and it can even create hollow cavities within the prints,” says Meyer, noting that the upgraded DIY printer can print living materials with more than 100 layers.
“This opens up possibilities to make structures that have a high surface-to-volume ratio, so that the embedded bacteria can more efficiently receive signals or nutrients from the environment and can excrete any useful products much more rapidly into their surroundings,” she adds.
Researchers also developed a support gel called a slurry that the bioprinter prints into, which holds up bio-ink and helps it solidify quickly and at any height.
Two types of slurry were created: one for easy removal of the print and one for incubation that allows microbes in the bioprints to stay alive in the slurry for four or more weeks. In previous methods, the printed bacteria started to die after about nine days.
The new slurry could have a significant impact on the research of biofilms—three-dimensional communities of microorganisms, such as bacteria, that adhere to surfaces—that can be both harmful and beneficial to humans.
For Meyer, the benefit of using different methods of incubation is the possibility “to create engineered biofilm materials that either have more biofilm characteristics, allowing study of and testing on medically relevant biofilm, or that have stronger mechanical properties, allowing them to be used for applications.”
For more information: ACS Applied Polymer Materials
Image: Anne S. Meyer’s lab has been making its own low-cost bioprinters for more than a decade, using them to print living structures to test new antibacterial and wastewater treatments along with other applications. Credit: URochester photo / J. Adam Fenster