Lippert Components Inc. (Lippert), Eklhart, Ind., announced it is upgrading the formula for all powder coatings on chassis out of the Goshen and Middlebury locations, which serves all of its OEM customers. The change comes as a result of two industry leaders, Lippert and AkzoNobel, Netherlands, collaborating to raise the bar in product performance and innovative manufacturing processes. The powder coating technology and performance is the best AkzoNobel has to offer, ultimately taking Lippert chassis products to new heights.
The Road Defense powder coating formula is designed to provide a more uniform density and give the chassis more protection against the elements. It has endured rigorous testing to ensure superior strength, durability and resistance to corrosion, fading, weathering, humidity and more. Additionally, on top of its ability to provide high-end protection, it features a sleek, modernized appearance.
There are a number of pivotal characteristics of the new powder coating that set it apart, including its texture instead of the traditional high-gloss black. Other key features and benefits include:
- 3x more resilient to salt spray and humidity
- 5x improved weathering for reduced fading and chalking
- 2x more resistant to chipping and cracking
- 4x more uniformed coverage for increased protection and performance
- 3x heavier coating for improved durability and reduced touch-ups
- Enhanced cyclic corrosion score to withstand harsh weather environments
The Road Defense chassis powder coating will initially be Indiana-based, and production will begin in early Q1.