Paper battery
Scientists found a whole new use for copier paper. Nanotubes + ink + paper = instant battery! These batteries will be 10 times more powerful than LiPos, easier to dispose of, lighter, and less expensive to make! According to Stanford University, Calif., researchers, when ordinary office paper coated is coated with an inky layer of carbon nanotubes or nanowires, it will become lightweight, flexible and highly conductive battery or superconductor.