United States Capitol Dome Restoration




Repair and Refurbishment of the U.S. Capitol Dome

Did you know that the dome of the U.S. Capitol building in Washington is made of nine million pounds of cast iron? Built during the 1850’s to 1860’s, it is now in the midst of an extensive repair/refurbishment program that is scheduled to be completed by January 2017. 