Watch self-healing material in action
A new electronic material can heal all its functions automatically—even after breaking multiple times. This material could improve the durability of wearable electronics. “Wearable and bendable electronics are subject to mechanical deformation over time, which could destroy or break them,” says Qing Wang at Penn State. “We wanted to find an electronic material that would repair itself to restore all of its functionality, and do so after multiple breaks.”