How Titanium is Made by the Kroll Process




Most titanium is now made by the Kroll process, in which titanium dioxide is reacted with chlorine to form titanium etrachloride, which is then reacted with magnesium to strip away the chlorine and leave behind the pure metal. Because the metal has multitudes of pores, it is called titanium “sponge. The sponge is then cast into ingots.