Using Machine Learning to Develop New Materials




Researchers at Delft University of Technology (TU Delft) have developed a new material without conducting any experimental tests at all. They designed a supercompressible but strong material using artificial intelligence (AI). “AI gives you a treasure map and the scientist needs to find the treasure,” says Miguel Bessa, lead researcher. Video courtesy of TU Delft, the Netherlands.