Thermal Spray Aluminum Coating Application and Adhesion Testing – ARC




This video demonstrates surface preparation, thermal spray aluminum by ARC spray with ARC150, thickness testing by DFT gauge, and adhesion testing of a typical pre-qualification operator test plate.
 