How to heat treat hand tools
This video from electronicsNmore is an easy tutorial on how to easily and properly heat treat and temper hand tools, and small knives. All that is required is a propane or MAPP gas torch, cold water, motor oil, mill file or bench grinder, and 220 grit sandpaper or a small wire brush.