Scientists create ’shape-shifting’ metal robot which melts through bars




Engineers have designed miniature robots that rapidly and reversibly shift between liquid and solid states. Scientists from Carnegie Mellon University in Pittsburgh took gallium, a metal that melts at room temperature, and enriched it with magnetic particles. When an alternate magnetic field is run through the metal, it can melt, move, and re-form.