A group of scientists at the Institute for Solid State Physics at TU Wien (Vienna) are conducting research on special metallic materials—small crystals that have been specially grown in the laboratory. According to lead researcher, Prof. Andrej Pustogow “These crystals can take on the properties of a metal, but if you vary the composition just a little bit, we are suddenly dealing with an insulator that no longer conducts electricity and is transparent like glass at certain frequencies.”
Right at this transition, one encounters an unusual phenomenon: the electrical resistance of the metal becomes extremely large—larger, in fact, than should be possible at all according to conventional theories. “Electrical resistance has to do with the electrons being scattered at each other or at the atoms of the material,” explains Andrej Pustogow. According to this view, the greatest possible electrical resistance should occur if the electron is scattered at every single atom on its way through the material—after all, there is nothing between an atom and its neighbor that could throw the electron off its path. But this rule does not seem to apply to so-called “bad metals.” They show a much higher resistance than this model would allow.
The key to solving this puzzle is that the material properties are frequency-dependent. “If you just measure the electrical resistance by applying a DC voltage, you only get a single number—the resistance at zero frequency,” says Andrej Pustogow. “We, on the other hand, made optical measurements using light waves with different frequencies.”
This showed that the “bad metals”—ones whose metallic states have extremely poor electrical conductivity—are not so “bad” after all. At low frequencies, they hardly conduct any current, but at higher frequencies they behave as one would expect from metals. The research team considers tiny amounts of impurities or defects in the material, that can no longer be adequately shielded by a metal at the boundary to an insulator, as a possible cause. These defects can cause some areas of the crystal to no longer conduct electricity because there the electrons remain localized in a certain place instead of moving through the material. If a DC voltage is applied to the material so that the electrons can move from one side of the crystal to the other, then virtually every electron will eventually hit such an insulating region and current can hardly flow.
At high AC frequency, on the other hand, every electron moves back and forth continuously—it does not cover a long distance in the crystal because it keeps changing direction. This means that in this case many electrons do not even come into contact with one of the insulating regions in the crystal.
“Our results show that optical spectroscopy is a very important tool for answering fundamental questions in solid-state physics,” says Andrej Pustogow. “Many observations for which it was previously believed that exotic, novel models had to be developed could very well be explained by existing theories if they were adequately extended. Our measurement method shows where the additions are necessary.” Already in earlier studies, Prof. Pustogow and his international colleagues gained important insight into the boundary region between metal and insulator, using spectroscopic methods, thus establishing a fundament for theory.
Image – View inside the optical spectrometer used in research on metallic materials. Courtesy of the Vienna University of Technology.
************
For more information: