Researchers at ETH Zurich, Switzerland, have developed a new type of laminate that changes color as soon as the material is deformed. This way, the materials researchers can kill two birds with one stone: a lightweight composite material that inspects itself.
Lightweight construction has found its way into many areas, especially automotive manufacturing, shipbuilding, and aircraft construction. In addition to traditional lightweight metals such as aluminum, magnesium, or titanium, load-bearing applications are increasingly featuring composite materials. This is driving a concurrent need to develop new techniques and methods for the early detection of damage to or even the possible failure of such as yet understudied materials.
Researchers from the Complex Materials Group at ETH Zurich, working in collaboration with researchers from the University of Fribourg, have now adopted an approach that has recently garnered attention in materials research: they have created a lightweight material that uses a color change to indicate internal deformation and thus possible material failure at an early stage. Composed of individual layers, their laminate is translucent, break resistant, and yet very lightweight.
The laminate is composed of alternating layers of a plastic polymer and artificial nacre or mother-of-pearl. The latter is a specialty of the Complex Materials Laboratory and is modeled on the biological example of the mussel shell. It consists of countless glass platelets arranged in parallel, which are compacted, sintered and solidified using a polymeric resin. This makes it extremely hard and break resistant.
The second layer consists of a polymer to which the researchers added an indicator molecule synthesized specifically for this application at the University of Fribourg. The molecule is activated as soon as the polymer experiences stretching forces, and this changes its fluorescence. The more the material stretches and the more of these molecules are activated, the more intense the fluorescence becomes.
“We used fluorescent molecules because you can measure the increase in fluorescence very well and you don’t have to rely on subjective perception,” says Tommaso Magrini, lead author of the study, which was recently published in the journal ACS Applied Materials and Interfaces. The system could also have been set up to produce a color change that would be directly perceptible from the outside. But: “The perception of colors is subjective and it is difficult to draw conclusions about changes in the material,” Magrini says.
With the help of fluorescence, the researchers can now identify overstressed areas within the composite material even before fractures form. This allows early detection of vulnerable areas in a structure before catastrophic failure occurs. One possible application of the novel laminate is in components in the load-bearing structures found in buildings, aircraft or vehicles, where it is essential to detect their failure at an early stage.
However, it remains to be seen whether and how the material can be produced on an industrial scale. So far, it exists only at laboratory scale as a proof of concept.
Image – A crack, not visible from the outside, forms and propagates inside the material. At the first sign of damage, it begins to fluoresce. Courtesy of ACS Appl. Mater. Interfaces.
************
For more information: