Unplanned discovery could lead to future pivotal discoveries in batteries, fuel cells, devices for converting heat to electricity, and more.
Mercouri Kanatzidis, professor at Northwestern University with a joint appointment in the U.S. Department of Energy’s (DOE) Argonne National Laboratory, was searching for a new superconductor with unconventional behavior when he made an unexpected discovery. It was a material that is only four atoms thick and allows for studying the motion of charged particles in only two dimensions. Such studies could spur the invention of new materials for a variety of energy conversion devices.
Kanatzidis’s target material was a combination of silver, potassium, and selenium (α-KAg3Se2) in a four-layered structure like a wedding cake. These 2D materials have length and width, but almost no thickness at only four atoms high. Superconducting materials lose all resistance to the movement of electrons when cooled to very low temperatures.
“Much to my disappointment, this material was not a superconductor at all, and we could not make it one,” said Kanatzidis, who is a senior scientist in Argonne’s Materials Science Division (MSD). “But much to my surprise, it turned out to be a fantastic example of a superionic conductor.”
In superionic conductors, the charged ions in a solid material roam about just as freely as in the liquid electrolytes found in batteries. This results in a solid with unusually high ionic conductivity, a measure of the ability to conduct electricity. With this high ionic conductivity comes low thermal conductivity, meaning heat does not pass through easily. Both of these properties make superionic conductors super materials for energy storage and conversion devices.
The team’s first clue that they had discovered a material with special properties was when they heated it up to between 450 and 600 degrees Fahrenheit. It transitioned into a more symmetrical layered structure. The team also found this transition to be reversible when they lowered the temperature, then raised it again into the high-temperature zone.
Scientists have been searching for some time to find an exemplary material to investigate ion movement in 2D materials. This layered potassium-silver-selenium material appears to be one. The team measured how the ions diffused in this solid and found it to be equivalent to that of a heavily salted water electrolyte, one of the fastest known ionic conductors.
While it is too early to tell if this particular superionic material might find practical application, it could immediately serve as a crucial platform for designing other 2D materials with high ionic conductivity and low thermal conductivity.
Studies with this superionic material could also be instrumental for designing new thermoelectrics that converts heat to electricity in power plants, industrial processes, and even exhaust gas from automobile emissions. And such studies could be used for designing membranes for environmental cleanup and desalting of water.
For more information: Argonne National Laboratory