Researchers explore the microworld using haptic optical tweezers

What if you could reach through a microscope to touch and feel the microscopic structures under the lens? In a breakthrough that may usher in a new era in the exploration of the worlds that are a million times smaller than human beings, researchers at Université Pierre et Marie Curie in France have unveiled a new technique that allows microscope users to manipulate samples using a technology known as “haptic optical tweezers.

New sensor improves lifespan of high-temperature engines

A temperature sensor developed by researchers at the University of Cambridge, UK, could improve the efficiency, control, and safety of high-temperature engines. The new sensor, or thermocouple, reduces drift by 80% at temperatures of 1200°C, and by 90% at 1300°C, potentially doubling the lifespan of engine components. The thermocouple withstands oxidization and minimizes any contamination to the wires from the metallic sheath.

Hardide develops polycrystalline diamond coating for drilling tools

Hardide Coatings Ltd., UK, has developed a TSP (thermally stable polycrystalline) diamond coating to extend the life and improve the performance of drilling tools operating in extremely abrasive environments. This is the first successful high-performance coating that can withstand the higher temperatures associated with TSP brazing, extreme loads, and aggressive media.

Dow Corning joins Imec to advance its temporary wafer-bonding solution

Dow Corning, Midland, Mich., announces that it is among the newest members of Imec, San Francisco. One of the key challenges is the bonding of the device wafer to a carrier wafer prior to wafer thinning, and the safe debonding of the thin wafer after completion of backside processing. This was Dow Corning’s goal when designing its temporary bonding solution, aimed at simple processing with a bi-layer concept comprising an adhesive and a release layer.

Tin-silver plating chemistry designed for lead-free solder bump plating

Dow Electronic Materials, Marlborough, Mass., announces availability of its Solderon BP TS 6000 tin-silver plating chemistry for lead-free solder bump plating applications. In copper pillar capping applications, it forms a smooth, micro-void free interface post reflow. It features enhanced plating performance, bath stability, and ease of use, thereby enabling the industry’s widest process window with the most robust process flexibility and a competitive cost of ownership.