Stronger materials could bloom with new images of plastic flow

Scientists from the Department of Energy’s SLAC National Accelerator Laboratory have captured high-resolution images of a tiny aluminum single-crystal sample as it transitioned from elastic to plastic state. The images will allow scientists to predict how a material behaves as it undergoes plastic transformation within five trillionths of a second of the phenomena occurring.