Carbon control during sintering improves quality of MIM parts

Linde North America Inc., Murray Hill, N.J., and Megamet Solid Metals, Earth City, Mo., a custom metal-injection molding company, have shown that the quality of metal-injection-molded parts could be significantly enhanced by following Linde’s advanced Sinterflex atmosphere control system.

ESA Solar Orbiter animation 2012

Solar Orbiter on a Mission to Study the Sun Solar Orbiter, a project of the European Space Agency in collaboration with NASA, aims to make significant breakthroughs in our understanding both of how the inner heliosphere of the sun works, and of the effects of solar activity on it. The spacecraft will take a unique […]