Graphene enhances XPS

X-ray photoelectron spectroscopy (XPS) is one of the most sensitive and informative surface analysis techniques available.

MIT researchers develop “miniscule” shape memory ceramic

A team at the Massachusetts Institute of Technology, Cambridge, together with two collaborators in Singapore, has reportedly developed a way to make minuscule ceramic objects that are not only flexible, but also have a “memory” for shape.