By creating atomic chains in a 2D crystal, researchers at Penn State believe they have found a way to control the direction of materials properties in two and three dimensional crystals with implications in sensing, optoelectronics, and next-generation electronics applications.
Carbon fiber project partnership
Pulsed electron beams enable rapid deposition of Ga-La-S thin films
The University of Southampton, England, announces that a research group has developed a rapid deposition technology in which pulsed beams of electrons break up a gallium-lanthanum-sulfur (GLS) glass target material and deposit it as a thin film onto a substrate at a rate greater than 0.2 microns/minute.