World’s smallest diamonds make tiny wires

Scientists at Stanford University, Menlo Park, Calif., and the Department of Energy’s SLAC National Accelerator Laboratory discovered a way to use diamondoids—the smallest possible bits of diamond—to assemble atoms into the thinnest possible electrical wires, just three atoms wide.

Surgical pins change color with strain

Engineers at Tufts University, Medford, Mass., created a new format of solids made from silk protein that can be preprogrammed with biological, chemical, or optical functions, such as mechanical components that change color with strain, deliver drugs, or respond to light.

Alcoa secures contract to export bauxite from its Western Australia mine

Alcoa Corp., Pittsburgh, announces that Alcoa World Alumina and Chemicals has secured its first major third-party contract to supply approximately 400,000 bone dry metric tons (bdmt) of bauxite from its Huntly mine in Western Australia, furthering Alcoa’s strategy to grow its third-party bauxite business.