Buehler, Lake Bluff, Ill., offers Diamet hardness testing software, which includes an automatic symmetry calculation for both Knoop and Vickers as a standard feature.
Plasma nitriding is a surface-hardening process in which glow-discharge technology introduces nascent (atomic) nitrogen into the surface of a metal part for subsequent inward diffusion
Lead-acid batteries are still the best choice for starting cars and trucks. The Engineer Guy explains why this is true, in spite of the development of many other battery types.
ASB Industries, Barberton, Ohio, announces that an industry-university team of researchers recently concluded a project that examined the relationship between lubricant additives and ferrous and nonferrous surfaces.