Credible Reference Information Makes All the Difference Purchase your resources from the most trusted materials science publisher in the world. Build on your technical knowledge with ASM’s publications, peer-reviewed by our industry experts. Our reference materials keep you at the leading edge of materials science.

Carbon control during sintering improves quality of MIM parts

Linde North America Inc., Murray Hill, N.J., and Megamet Solid Metals, Earth City, Mo., a custom metal-injection molding company, have shown that the quality of metal-injection-molded parts could be significantly enhanced by following Linde’s advanced Sinterflex atmosphere control system.