International Molybdenum Association publishes emissions study

The International Molybdenum Association (IMOA), London, has published a study demonstrating that lightweight components manufactured from advanced high-strength steel (AHSS) can reduce attributable greenhouse gas emissions by around 29% compared with traditional component designs.

How It’s Made Magnets

This video from the Science/Discovery Channel shows how permanent magnets are made by melting together copper, cobalt, sulfur, nickel, iron, aluminum, and titanium.