ChromX 9000 concrete rebar provides five times the corrosion resistance of carbon steel
Al-Fe Heat Treating offers glycol quenching of aluminum for precise control
GlobalFoundries to acquire IBM’s global semiconductor business
IBM, Armonk, N.Y., and GlobalFoundries, Santa Clara, Calif., today announced that they have signed a Definitive Agreement under which GlobalFoundries plans to acquire IBM’s global commercial semiconductor technology business, including intellectual property, world-class technologists and technologies related to IBM Microelectronics, subject to completion of applicable regulatory reviews.
Samsung to invest $14.7 billion in new semiconductor fab
SEMI announces silicon wafer shipment forecast