TSMC plans to spend $35B in Arizona fab

Upping its commitment to its state-of-the-art wafer fab in Arizona, Taiwan Semiconductor Manufacturing Corp. (TSMC), Taiwan, is reported to be investing some $35 billion in the U.S. manufacturing facility, almost tripling the original $12 billion it originally committed.