A University of Minnesota-led team has developed a first-of-its-kind, breakthrough method that makes it easier to create high-quality metal oxide thin films out of “stubborn” metals that have historically been difficult to synthesize in an atomically precise manner. This research paves the way for scientists to develop better materials for various next-generation applications including quantum computing, microelectronics, sensors, and energy catalysis.
“This breakthrough represents a significant advancement with far-reaching implications in a broad range of fields,” said Bharat Jalan, senior author on the paper and a professor in the College of Science and Engineering. “Not only does it provide a means to achieve atomically precise synthesis of quantum materials, but it also holds immense potential for controlling oxidation-reduction pathways in various applications including catalysis and chemical reactions occurring in batteries or fuel cells.”
“Stubborn” metals oxides, such as those based on ruthenium or iridium, play a crucial role in numerous applications in quantum information sciences and electronics. However, converting them into thin films has been a challenge for researchers due to the inherent difficulties in oxidizing metals using high-vacuum processes.
While attempting to synthesize metal oxides using conventional molecular beam epitaxy, a low-energy technique that generates single layers of material in an ultra-high vacuum chamber, the researchers stumbled upon a groundbreaking revelation. They found that incorporating a concept called “epitaxial strain”—effectively stretching the metals at the atomic level—significantly simplifies the oxidation process of these stubborn metals.
“The current synthesis approaches have limits, and we need to find new ways to push those limits further so that we can make better quality materials,” said Sreejith Nair, first author of the paper and a Ph.D. student in the College of Science and Engineering. “Our new method of stretching the material at the atomic scale is one way to improve the performance of the current technology.”
Although the research team used iridium and ruthenium as examples, their method has the potential to generate atomically precise oxides of any hard-to-oxidize metal.
The researchers worked with collaborators at Auburn University, the University of Delaware, Brookhaven National Laboratory, Argonne National Laboratory and fellow University of Minnesota Professor Andre Mkhoyan’s lab to verify their method.
“When we looked at these metal oxide films closely using very powerful electron microscopes, we captured the arrangements of the atoms and determined their types,” Mkhoyan explained. “Sure enough, they were nicely and periodically arranged as they should be in these crystalline films.”
For more information: Nature Nanotechnology
Image: Professor Bharat Jalan and Ph.D. candidate Sreejith Nair. Credit: University of Minnesota