Poster Session
Explore the latest advances in Suspension and Solution Thermal Spray (S&STS) technologies and Environmental Barrier Coatings (EBCs) at the TS4E 2026 Poster Session. This interactive session provides an opportunity for researchers and industry professionals to share innovative work, exchange ideas, and connect with experts from around the world. Early Stage Researchers are especially encouraged to participate and showcase their contributions to the future of advanced coatings.
Razieh Alikhanifaradonbeh, Tampere University
Icephobic Polyethylene/Carbon Coating by Dual Suspension-Powder Flame Spray TechniqueIcephobic Polyethylene/Carbon Coating by Dual Suspension-Powder Flame Spray Technique
Ameey Anupam, University West
Solution Precursor Plasma Spraying as a One-step Route for Depositing Refractory High-Entropy Oxide Coatings
Margherita Cescon, University of Modena and Reggio Emilia
Mechanical and Chemical Performance of Multilayered EBCs with Graded YbMS/YbDS Compositions
Ali Eskandari, University West
Toward Ultra-High Porous Gadolinium Zirconate Thermal Barrier Coatings by Suspension Plasma Spraying
Ewa Filipkowska, Wroclaw University of Science and Technology
Challenges in the development of thermally sprayed self-healing thermal barrier coatings
Ebru Gyoktepeliler Akin, IKMT, University of Stuttgart
Oxidation Behavior of HVSFS Sprayed TiN/Al₂O₃ Composite Coatings and Its Influence on Coating Properties
Ruhama Hasanov, FRAUNHOFER IWS
Suspension formulation and thermal spray deposition of modified TiO₂-based photocatalyst coatings for visible-light water splitting
Gilles Mariaux, University of Limoges, CNRS, IRCER
Advanced modelling of Suspension Plasma Spraying: focus on the physical treatment of the suspension
Sara Mokhlesi, IKMT – University of Stuttgart
Inconel 625 coatings via Suspension-HVOF for resistance heating: Influence of oxygen scavengers
Jade Orlandi, IMERYS/IRCER
Comparative study of particle behavior in aqueous and ethanol-based suspensions in suspension plasma spraying and the influence of powder chemistry from micrometric to nanometric scales
Karolina Płatek, Wroclaw University of Science and Technology
Comparative Study of TiO2 Photocatalytic Coatings Deposited by SPPS and SPS Using an Axial III Plasma Torch
Pavan Ravulaparthy, U.S. Department of Energy
Computationally Guided EBCs for High Temperature, Fuel Flexible sCO₂ Turbine Cycles—A DOE Perspective
Andrii Rednyk, Institute of Plasma Physics of the Czech Academy of Sciences
Liquid Plasma Sprayed Electrodes for Solid Oxide Fuel Cells (SOFCs)
Kieron Robinson, University of Nottingham
Suspension plasma spraying of GdPO4 coatings: influence of process parameters on microstructure and performance
Benjamin Rong Sheng Gan, University of Nottingham
Impact of Silica loss on the microstructure, mechanical performance, and CMAS resistance of a Suspension Plasma Sprayed YbDS coating
Zhoukun Shi, Université de technologie de Belfort Montbéliard (UTBM)
Comparison of suspension plasma sprayed coatings fabricated with two torch configurations (conventional and cascade) and two injection methods (mechanical and atomizer)
Kaito Takagi, TOCALO Co., Ltd
Microstructural Control and Functional Properties of Columnar YSZ Coatings Deposited by Suspension Plasma Spraying