Quintus, Västerås, Sweden, has supplied a Hot Isostatic Press (HIP) to Wallwork Group’s new HIP Centre stated to open in Bury, North Manchester, England, in September 2023. The press is the model QIH 173L M URC, equipped with Quintus’ proprietary uniform rapid cooling (URC), a feature that delivers the high material uniformity required of parts designed formission-critical applications, while enabling increased productivity with optimal temperature control.
Operating at a maximum temperature of 1250°C (2282°F) and pressure of 207 MPa (30,000 psi), the technologically advanced press has a work zone measuring 800 mm (34.6 inches) in diameter and 2550 mm (100.4 inches) high, and a capacity of over 7000 kg (15,432 lbs) per cycle.