Researchers from Tokyo Metropolitan University have found new ways of controlling how heat flows through thin materials by stacking atomically thin layers of atoms into van der Waals heterostructures. By comparing different stacks of different materials, or even the same material after heat treatment, they found that weak coupling and mismatch between layers helped significantly reduce heat transport. Their finding promises sensitive control of heat flow at the nanoscale in thermoelectric devices.
A team led by Professor Kazuhiro Yanagi of Tokyo Metropolitan University has been working on ways to produce and handle ultrathin layers of a class of materials known as transition metal dichalcogenides. Here, they took layers of molybdenum disulfide and molybdenum diselenide a single atom thick and stacked them together into layers of four (4L films). The layers could be coupled together in separate ways. The team’s unique, gentle way of transferring large single atom-thin sheets allowed them to create stacks of layers bound together by van der Waals forces. They could also be strongly bound by more conventional techniques, specifically chemical vapor deposition (CVD). This gives rise to several permutations for how isolated layers could be put together, and potentially control how heat gets through them.
By using a special coating technique, they were able to detect how miniscule amounts of heat flowed past these stacks with good accuracy. Firstly, they found that layers strongly bound by CVD let through significantly more heat than their loosely bound counterparts. This effect could be partially reversed by annealing weakly held layers, making the binding stronger and improving upon the transport of heat. Furthermore, they compared stacks of four molybdenum sulfide layers to a “lasagna”-like structure made of alternating layers of molybdenum sulfide and molybdenum selenide. Such heterostructures had an artificial structural mismatch between adjacent layers of atoms which led to significantly lower levels of heat transfer, more than ten times less than with strongly bound layers.
The team’s findings not only demonstrate a new technical development but provide general design rules on how one might control how heat flows at the nanoscale, whether you want more or less flow. These insights will lead to the development of ultrathin, ultralight insulators as well as new thermoelectric materials, where heat might be effectively channeled for conversion into electricity.
For more information: ACS Publications