Nitrex Vacuum, Quebec, has delivered two large-capacity nitriding systems to the Italian gear manufacturer, Capi Group. Capi has been using Nitrex systems since 2018 and the new systems are expected to boost their nitriding/nitrocarburizing capacity.
The Capi Group now owns four pit-type nitriding/nitrocarburizing furnaces of the same model type and size – the large heavy-duty NX-1230 furnace with a load capacity of 11,570 lb (5,250 kg), which uses Nitreg and Nitreg-C technologies for results that are guaranteed to be repeatable and consistent. The addition of accelerated cooling technology shortens the cooling period, allowing for faster output. The NX furnace design assures +/-3°C temperature homogeneity in the retort. The eco-friendly IN-500 exhaust neutralizer supports a clean and green operation.
Read further here.