New ArcX center North America inaugurated in Texas

The new ArcX facility in Houston Texas, from Höganäs, Sweden, inaugurated in March 2023, is set to further strengthen the company’s position in the surface coating market and will provide state-of-the-art technical support to its surface coating customers.

Titomic enters next step of commercialization with Boeing

Titomic Limited, Australia, has received a purchase order from Boeing Space, Intelligence, and Weapons Systems for AUD 132,174 to continue flight qualifications of Titomic Kinetic Fusion manufactured components initiated in 2021.

One Minute Mentor: Vacuum Furnaces

The demands on vacuum-hardening technology have changed in recent decades. One of the most important considerations that must be met is the accomplishment of highest dimensional stability with optimal microstructural properties and minimal change of the surface of the workpieces.  Minimizing exposure to air during the heat treatment by reducing the quantity of oxygen in […]