3D printing creates and assesses alloys

A 3D printer allows researchers at Ames Laboratory, Iowa, to rapidly create and assess alloys of varying composition to find just the right combination to produce materials with the desired characteristics.

Buehler upgrades Wilson DiaMet hardness testing software

Buehler, Lake Bluff, Ill., announces that it has extensively upgraded its Wilson DiaMet hardness testing software with features designed to facilitate and accelerate specific applications, such as the documentation of the hardness distribution in welds, or the depth of hardening in induction-hardened workpieces or in objects hardened with conventional processes.