FEI, Hillsboro, Ore., introduces the DualBeam plasma-focused ion beam (PFIB) for sample preparation, electrical fault isolation, and electrical failure analysis on sub-20nm semiconductor devices.
DCG Systems, Fremont, Calif., has acquired the assets of MultiProbe, the leading provider of atomic force-based nanoprobe solutions for the semiconductor industry.
Researchers from Stanford University, Stanford, Calif., report that they have developed graphene sheathing material for the copper wires in computer chips.
Researchers from North Carolina State University, Raleigh, report that they have fabricated stretchable transparent conductors that work because of their “nano-accordion” design.
The Technical University of Munich (TUM) announces that its researchers have printed razor-thin polymer electrodes with improved electrical properties.