Ipsen USA, Cherry Valley, Ill., reports that California Brazing recently purchased its third vacuum aluminum brazing (VAB) furnace from Ipsen, to expand capacity and manufacture a variety of aluminum-brazed assemblies.
Continue readingNucor to acquire Gerdau’s cold-drawn steel bar assets in Ohio and Georgia
Nucor Corp., Charlotte, N.C., has agreed to acquire Gerdau Long Steel’s Bright Bar assets located in Orrville, Ohio, and Cartersville, Georgia, which manufacture cold-drawn steel bars and have a combined production capacity of 75,000 tons per year.
Continue readingAmbrell launches Ekoheat with VPA for improved induction processes
Ambrell, Scottsville, N.Y., has launched a line of Ekoheat products featuring Versatile Performance Architecture (VPA), which enables a product to integrate into manufacturing systems or to function as a stand-alone induction heating solution.
Continue readingAir Force selects Northrop Grumman to build new long-range bomber
The U.S. Air Force has selected Northrop Grumman Corp., Falls Church, Va., the company that developed the B-2 Spirit stealth bomber, to deliver the new Long-Range Strike Bomber, which is also to be stealthy.
Continue readingTitanium strength and ductility grow when large grains are added to microstructure
A team from North Carolina State University, Raleigh, and the Chinese Academy of Sciences announces that titanium strength and ductility are both increased when large grains are added to an ultrafine-grain matrix.
Continue readingMessage from the President: Thermal Spray Leaders Newly Elected ASM Fellows
Good news! Two leaders of our thermal spray community were elected ASM Fellows for their distinguished contributions to materials science and engineering.
Continue readingLockheed Martin closes acquisition of Sikorsky Aircraft
Lockheed Martin, Bethesda, Md., has closed its acquisition of Sikorsky Aircraft, a world leader in military and commercial rotary-wing aircraft.
Continue readingOerlikon SinplexPro plasma spray gun allows standardizing coating parameters
Oerlikon Metco, Switzerland, offers its SinplexPro plasma spray gun, which brings the benefits of cascading arc technology to existing plasma spray systems, and allows applicators to standardize coating parameters across multiple spray systems.
Continue readingSlippery anti-fouling nanoporous tungsten oxide coating strengthens steel
Harvard University, Cambridge, Mass., reports that a research team has developed a slippery anti-fouling coating made from nanoporous tungsten oxide that also makes steel stronger and more durable.
Continue readingSilver nanoparticles in polymer coating prevent infections in dental implants
Researchers at the Fraunhofer Institute, Germany, have reportedly developed DentaPlas, an antimicrobial coating for dental implants that consists of three layers, with two plasma polymer layers surrounding a center layer of silver nanoparticles.
Continue readingGrant awarded to study key energy materials
Researchers at the University of Arkansas, Fayetteville, will use a $374,621 federal grant to investigate fundamental properties of materials that are considered key to advances in energy generation, storage, and conversion.
Continue readingHarvesting more energy from photons
Quantum process increases the number of electrons produced when light strikes a metal-dielectric interface
Continue readingHeat treat 2015 finishes with a “bang!”
ASM International, Materials Park, Ohio, announces that the ASM Heat Treating Society Conference and Exposition (Heat Treat 2015) in Detroit, co-located with the American Gear Manufacturer’s Association Gear Expo, attracted over 7000 heat treating and gear professionals from all over the world.
Continue readingHeat Treat 2015 Finishes with a “BANG!”
The ASM Heat Treating Society Conference and Exposition (Heat Treat 2015) took place in late October in Detroit. The three-day event, co-located with the American Gear Manufacturer’s Association Gear Expo, attracted over 7000 heat treating and gear professionals from all over the world, including an equipment exhibition featuring 202 companies in 288 booths.
Continue readingLincoln Electric to invest $30 million to build Welding Technology Center
The Lincoln Electric Co., Cleveland, Ohio, announces that it is investing approximately $30 million in a new Welding Technology Center on its campus in Euclid, Ohio.
Continue readingIpsen predictive maintenance for heat treating furnaces cuts costs, optimizes operations
Ipsen, Cherry Valley, Ill., displayed the Titan 2.0 heat treating vacuum furnace and PdMetrics software platform for predictive maintenance at ASM International’s Heat Treat 2015 conference.
Continue readingVaporized foil actuator welding produces bonds 50% stronger
Engineers at Ohio State University, Columbus, report that they have developed vaporized foil actuator (VFA) welding, a technique that consumes 80% less energy than conventional techniques, yet produces bonds that are 50% stronger.
Continue readingASM Handbooks Online now includes Volume 5B: Protective Organic Coatings
ASM International, Materials Park, Ohio, recently released ASM Handbooks Online, which features the addition of ASM Handbook, Volume 5B: Protective Organic Coatings.
Continue readingUnraveling structural ambiguities in lithium-rich transition metal oxides
Using complementary microscopy and spectroscopy techniques, researchers at say they have solved the structure of lithium- and manganese-rich transition metal oxides.
Continue readingNew welding technique welds “unweldable” metals
Engineers at The Ohio State University developed a new welding technique that consumes 80% less energy than a common welding technique, yet creates bonds that are 50% stronger—creating a huge impact on the auto industry.
Continue readingSSAB launches high-strength steels designed for auto chassis
SSAB, Sweden, announces that during the next 12 months it will release two hot-rolled advanced high-strength steel grades that exceed 800 and 1000 MPa in tensile strength for automobile chassis applications.
Continue readingSeco-Warwick case-hardening system reduces distortion in gears
Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.
Continue readingConstellium launches Aeral aluminum for aerosol cans
Constellium N.V., Amsterdam, has launched Aeral, an aluminum solution designed for making aerosol containers by the “drawn and ironed” technology currently used to produce beverage cans.
Continue readingPraxair, Atmosphere Engineering sign joint marketing agreement
Praxair Inc., Danbury, Conn., has signed an agreement with Atmosphere Engineering that will allow customers to access Praxair’s industrial gases, application technologies, and supply systems, as well as Atmosphere Engineering’s furnace control systems and sensors.
Continue readingOne Minute Mentor: Isothermal Transformation Diagram for Tool Steels
The graph shows the isothermal transformation diagram for the steel AISI 1075/DIN EN C75. Cooling curves show three process cycles for molten metal quenching in the time-temperature-transformation plots.
Continue readingBodycote expands hot isostatic pressing capacity
Bodycote, England, is expanding its high pressure Hot Isostatic Pressing (HIP) capability with the addition of a new mid-range vessel to increase its volume capacity.
Continue readingAMI Metals to provide flat-rolled aluminum plate for the F-35 Joint Strike Fighter
Reliance Steel & Aluminum Co., Los Angeles, announces that its subsidiary AMI Metals Inc., headquartered in Brentwood, Tennessee, has been awarded a multi-year contract by Lockheed Martin to provide aluminum flat rolled plate for the F-35 Joint Strike Fighter.
Continue readingNorsk Titanium orders three more machines to build titanium parts by Rapid Plasma Deposition
Reliance Steel & Aluminum Co., Los Angeles, announces that its subsidiary AMI Metals Inc., headquartered in Brentwood, Tennessee, has been awarded a multi-year contract by Lockheed Martin to provide aluminum flat-rolled plate for the F-35 Joint Strike Fighter.
Continue readingShimadzu high-speed video camera allows ten million frames per second
Shimadzu Scientific Instruments, Japan, announces the release of its new Hyper Vision HPV-X2 high-speed video camera that features ultra-high-speed recording at ten million frames-per-second.
Continue readingShimadzu high-speed video camera allows ten million frames per second
Shimadzu Scientific Instruments, Japan, announces the release of its new Hyper Vision HPV-X2 high-speed video camera.
Continue reading