Constellium publishes 2024 sustainability report outlining decarboConstellium publishes 2024 sustainability report outlining decarbonization and recycling milestonesnization and recycling milestones

Constellium, Paris, announced that it has released its 2024 Sustainability Report, detailing progress toward its environmental, social, and governance (ESG) goals and reinforcing its commitment to building a sustainable, circular economy. The report highlights advancements in aluminum recycling, decarbonization initiatives, workplace safety, and gender equity.

Among the year’s key accomplishments is the opening of a €130 million recycling facility in Neuf-Brisach, France, which increases the company’s global recycling capacity to more than 750,000 metric tons per year. The site enhances automotive and packaging recycling by 75%, reduces annual carbon emissions by approximately 400,000 metric tons CO₂eq, and integrates biodiversity assessments and energy-efficient technologies.

In line with its decarbonization strategy, Constellium also decommissioned its final coal-powered energy source at the Singen plant in Germany. The closure is projected to cut direct greenhouse gas emissions at the site by more than 25% between 2021 and 2025.

Further emphasizing innovation, Constellium completed its first industrial-scale hydrogen casting at its C-TEC R&D facility in July. This pilot project substituted natural gas with hydrogen to produce a 12-metric-ton aluminum slab for electric vehicle applications, showcasing the potential of hydrogen to lower emissions in industrial processes.

The company’s sustainability efforts have been validated through independent certifications. All Constellium operations were certified under the Aluminium Stewardship Initiative’s Performance Standard v3.0, recognizing best practices in emissions reduction, waste management, and human rights. Constellium also maintained a Gold rating from EcoVadis and an AA rating from MSCI for its ESG performance.

Jean-Marc Germain, chief executive officer, emphasized aluminum’s role in advancing low-carbon manufacturing, noting its recyclability and efficiency in lightweight applications. He reiterated the company’s commitment to delivering sustainable solutions across the aluminum value chain.

Read further here: Constellium’s sustainability page.

NUTEC Bickley secures major contract for advanced ceramic core sintering kiln

NUTEC Bickley, Monterrey, Mexico, announced that it has been awarded a contract to supply a four-car shuttle kiln to a leading global energy technology company. The kiln will support sintering of ceramic cores at the customer’s investment casting facility, with firing cycles ranging from 20 to 80 hours, depending on the core specifications.

The gas-fired shuttle kiln is engineered to operate at temperatures up to 2010°F (1100°C) and features a twin-deck kiln car setting. Each car offers setting dimensions of 47 inches long by 63 inches wide by 34 inches high (1.19m x 1.59m x 0.87m), delivering a total effective load volume of 230 cubic feet (6.55m³) across all four cars. The kiln is designed to handle an average total product weight of 970 pounds (440 kg).

Twelve individually controlled high-velocity nozzle-mix burners—firing in a staggered sequence above and below the load—enable optimal heat transfer and temperature uniformity. Each burner includes automatic ignition and a safety system.

The kiln incorporates NUTEC Bickley’s proprietary IMPS® combustion control system, which provides pulse control across eight independent temperature zones, alternating between high and low fire settings. The system allows programmable excess air levels during different stages of the cycle, enhancing fuel efficiency, process precision, and temperature uniformity without relying on constant excess air. IMPS also includes a cooling mode, introducing air through burners and dedicated nozzles for reduced cycle times.

The kiln’s insulation includes NUTEC’s patented Jointless® ceramic fiber system rated to 2600°F (1425°C), ensuring thermal efficiency and durability. Double-labyrinth refractory and insulation brick seals combined with sand seals reduce heat loss and cold air infiltration.

This project builds on NUTEC Bickley’s longstanding relationship with the customer, which includes the delivery of 15 furnaces and ovens over the past decade to its transformer manufacturing division. The award further underscores NUTEC Bickley’s reputation for delivering advanced thermal processing systems to global leaders in high-tech manufacturing.

Read further here: https://www.nutecbickley.com/

Fort Wayne Metals receives 2025 Moving the Needle award for workplace equity

Fort Wayne Metals, Fort Wayne, IN, announced that it has received the 2025 Moving the Needle Award and Bronze-Level honors from the Women’s Fund of Greater Fort Wayne. The recognition was presented at the annual Women in the Workplace Luncheon held on March 12 at the Parkview Mirro Center for Research and Innovation.

The Moving the Needle Award is given to the organization that demonstrates the most notable progress across four areas: leadership, compensation, benefits and policies, and recruitment and retention. The selection is based on data collected through the Women’s Fund’s annual Compass Survey, which evaluates local employers’ efforts toward achieving gender equity.

This year, a record 75 organizations participated in the survey, reflecting growing engagement across the community. Fort Wayne Metals’ recognition underscores its focused efforts to foster equitable workplace practices and support the advancement of women in its workforce.

Read further here.

Enovis releases 2024 Corporate Social Responsibility Report highlighting commitment to sustainability and community engagement

Enovis Corporation, headquartered in Wilmington, Delaware, announced the publication of its 2024 Corporate Social Responsibility (CSR) report, underscoring the company’s ongoing dedication to ethical practices, environmental stewardship, and social responsibility. ​

The report details Enovis’ initiatives aimed at fostering a positive global impact. Key highlights include the implementation of energy-efficient technologies across manufacturing facilities, resulting in a measurable reduction in the company’s carbon footprint. Additionally, Enovis has expanded its community outreach programs, partnering with local organizations to support health and education initiatives.​

The CSR report also emphasizes Enovis’ commitment to diversity and inclusion within its workforce, showcasing programs designed to promote equitable opportunities and a supportive work environment for all employees. By aligning its business strategies with sustainable and socially responsible practices, Enovis aims to contribute meaningfully to the well-being of its stakeholders and the broader community.​

For a comprehensive overview of Enovis’ CSR initiatives and achievements, the full 2024 report is available on the company’s website.

Read further here

Pyromaitre delivers integrated heat-treating solution to GKN driveline Mexico

Pyromaitre, Lévis, Québec, announced the completion of assembly for its P-208E oven system for GKN Driveline Mexico, marking a total of four systems delivered to the client. The company developed a fully integrated solution that includes a high-speed tempering furnace, a post-treatment cooling chamber, automated loading and unloading systems, and a smoke collection unit. Each component was configured to meet the customer’s specific production requirements.

Pyromaitre specializes in resolving convective heat transfer challenges with precision and efficiency. The company focuses on driving innovation and operational performance, aiming to be a recognized leader in stress relief and tempering solutions. Its core values—integrity, innovation, customer satisfaction, and teamwork—guide its approach to delivering high-performance thermal processing systems.

Read further:

Solar Atmospheres expands vacuum heat-treating capacity in Eastern Pennsylvania

Solar Atmospheres, Souderton, PA, announced the commissioning of two additional 2-bar vacuum furnaces at its Eastern Pennsylvania facility. The expansion is aimed at supporting increased demand from the aerospace and industrial gas turbine industries, as well as specialized hydride/dehydride processing of reactive metals such as titanium, tantalum, and niobium.

The newly installed furnaces, manufactured by Solar Manufacturing, feature large working hot zones measuring 45 inches wide by 45 inches high by 72 inches deep. They are rated for temperatures up to 2400°F and maintain a temperature uniformity of ±10°F, meeting the stringent requirements of high-performance heat treatment applications.

Mike Moyer, vice president of sales at Solar Atmospheres, noted that the new equipment, outfitted with the latest control systems from Solar Manufacturing, enhances operational efficiency and safety. He added that this expansion supports the company’s commitment to providing reliable service, competitive pricing, and fast turnaround times to its customers.

The additional capacity reflects Solar Atmospheres’ ongoing investment in advanced thermal processing technology to meet the evolving needs of its industrial and aerospace clients.

Read further here

 

Constellium and renault group complete r&d project advancing lightweight aluminium solutions

Constellium, Paris, announced the successful completion of the “ISA3” R&D project, an initiative launched in 2021 to advance lightweight aluminium solutions for automotive applications. Conducted in collaboration with Renault Group, ESI Group, the Institut de Soudure, and the University of Lorraine, the project was supported by a grant from the France Relance investment program. The research focused on developing cost-efficient, recyclable aluminium components to enhance vehicle performance and sustainability.

A key achievement of the project was the development of a lightweight aluminium door in partnership with Renault. Utilizing Constellium’s proprietary uni-alloy 6xxx rolled and extrusion-based solutions, the door design achieved a 14% weight reduction compared to existing aluminium doors used in compact battery electric vehicles. By employing a single alloy series, the project streamlined closed-loop recycling, reducing the door’s overall carbon footprint. This innovation resulted in a 33% reduction in Global Warming Potential (GWP), reinforcing the project’s emphasis on sustainability.

Beyond material advancements, the project also explored more efficient and flexible production processes to enhance performance while optimizing costs. Ludovic Piquier, senior vice president, manufacturing excellence and chief technical officer at Constellium, emphasized that the results highlight the company’s commitment to providing sustainable, high-performance aluminium solutions for the automotive sector.

Patrice Belliard, expert in flat products at Renault Group, noted that the project demonstrated how aluminium can support both weight reduction and cost efficiency in automotive manufacturing. Mathilde Chabin, manufacturing product director at ESI Group, added that the use of advanced pre-certification and validation technologies eliminated the need for physical prototypes, accelerating innovation while reducing costs and environmental impact.

The completion of Project ISA3 underscores the potential of aluminium to contribute to the automotive industry’s decarbonization efforts while delivering economic and environmental benefits.

Read further here. 

Furukuwa opens new laser processing laboratory in Aichi prefecture to advance industrial solutions

Furukawa Electric Co. Ltd., Tokyo, Japan, and Nichia Corp., Tokushima, Japan, announced that they have jointly opened the Cutting-Edge Laser Processing Solution Laboratory (CELL) in Kariya City, Aichi Prefecture. Located in a key hub of the automotive industry, the new facility is designed to accelerate the development of laser processing technologies and provide innovative solutions to industrial challenges.

The laboratory is equipped with Furukawa Electric’s advanced industrial lasers, including the newly developed 5kW blue laser (BR5000), which delivers world-leading brightness through optical fiber. Plans are in place to install the full range of Furukawa Electric’s industrial lasers, including the BRACE Series of Blue-IR hybrid lasers, enabling the lab to meet diverse customer requirements and expedite process testing and evaluations.

CELL is a collaborative effort between Furukawa Electric and Nichia, facilitating activities that span laser processing and light source development. This partnership will enable the two companies to propose next-generation laser solutions tailored to specific customer needs, with a particular focus on addressing the demands of copper processing for the electrification of mobility.

Both companies are committed to advancing laser technology and supporting the development of innovative production methods, contributing to the evolution of the automotive and related industries.

Read further here: 

TESCAN Group acquires EXpressLO LLC

TESCAN Group, a.s, Czech Republic, a leading global manufacturer of electron microscopes and advanced scientific instruments, has acquired EXpressLO LLC, Lehigh Acres, Fla., a provider of innovative FIB lift-out solutions for specimen preparation in STEM and other analytical techniques.

Continue reading

Seco/Warwick to supply Jetcaster technology to Turkish aviation company

Seco/Warwick, Meadville, Pa, announced that it will deliver a JetCaster induction vacuum furnace to a Turkish aviation company. The advanced furnace is designed for producing castings using directional solidification, single crystal, and equiaxed structure methods, as well as gas-cooled crystallization. The technology addresses the precision and quality requirements of aviation component manufacturing.

The JetCaster VIM50 DS/SC/EQ furnace, with a maximum load capacity of 50 kilograms, supports various crystallization techniques, offering flexibility and high performance. Its innovative Engineered Gas Cooling (DGCC) system shortens processing times while maintaining superior product quality, making it particularly suited to the stringent demands of the aviation sector.

Seco/Warwick’s CEO, Sławomir Woźniak, highlighted the increasing demand for the company’s vacuum metallurgy solutions within the aviation industry, noting its critical role in producing components for both civil and military aircraft. He emphasized the company’s collaboration with leading corporations globally to meet the sector’s high-quality standards.

This marks the first order of a melting furnace from this specific partner. Seco/Warwick customized the furnace design to accommodate future modifications, such as the addition of feeders for bulk materials or briquettes, ensuring adaptability to evolving production needs. The solution aims to enhance the partner’s production efficiency and innovation, solidifying its contribution to the aviation industry.

Read further here.

 

Constellium honored with supplier of the year award from stellantis for csr excellence

Constellium, Paris, announced that it has been awarded the Supplier of the Year Award by Stellantis, recognizing the company’s strong commitment to corporate social responsibility (CSR). This honor reflects Constellium’s dedication to high CSR standards in both its operations and supply chain, which has earned positive ratings from several international rating agencies. A long-standing supplier for Stellantis brands, Constellium provides aluminum body sheet products and extrusion-based structural solutions for various vehicle platforms across Europe and the U.S.

Constellium’s approach to sustainability has been acknowledged by independent organizations, including EcoVadis, the Carbon Disclosure Project (CDP), MSCI ESG Ratings, and ISS-Oekom. As a founding member of the Aluminium Stewardship Initiative (ASI), Constellium recently achieved ASI Performance Standard Certification for all global operations.

Ingrid Joerg, executive vice president and chief operating officer at Constellium, expressed pride in the award from Stellantis, noting that it underscores the company’s dedication to responsible purchasing and sustainable solutions. The award was presented at Stellantis’s annual event in Turin, Italy, where Maxime Picat, stellantis chief purchasing and supply chain officer, emphasized the critical role of suppliers in supporting Stellantis’s growth through their commitment to quality and collaboration. Constellium, dedicated to delivering sustainable aluminum products, publishes annual sustainability reports to highlight its progress and results in this area

Read further here.

One Minute Mentor : Phase Transformations in Numerical Simulation

Heat treatment of tool steels means several phase transformations. Every phase transformation must be described by start amount, end amount, and kinetics (change of phases depending on temperature and time). Start and end amount can be calculated with different thermodynamic software. For example, Thermocalc is well validated for tool steels. The most common method for determining the transformation kinetics of main phases (e.g. ferrite, austenite, martensite, bainite) is to use dilatometric investigations. TTT (time-temperature-transformation) diagrams obtained from dilatometer measurements can be easily implemented in HTS software. An example is shown in the figure. 

For more information, click on the link below (subscription required). Then scroll to Figure 14. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

Solar Manufacturing ships Mentor Pro furnaces for renewable energy applications

Solar Manufacturing, Sellersville, Pa., announced that it has shipped two Mentor Pro vacuum furnaces to a customer focused on developing advanced renewable energy technologies for large-scale industrial applications. The furnaces were selected after a collaborative process with the customer’s engineers, supported by the Research and Development team from Solar Manufacturing’s affiliate, Solar Atmospheres. The customer valued the furnace’s capabilities and compact design.

The Mentor Pro furnaces feature a molybdenum shielded hot zone, a maximum temperature capacity of 2500°F, and a workload capacity of up to 1000 pounds. They are equipped with SolarVac Essentials, a PLC-based control system, and include an internal gas quenching system with a 50 HP motor and variable frequency drive (VFD), offering flexibility in using nitrogen or argon gas for optimal metallurgical results. These features make the Mentor Pro well-suited for a variety of metallurgical applications in renewable energy development.

Read further here.

One Minute Mentor: Distortion of Ledeburitic Cold-Work Tool Steels

The different effects of steel composition on the dimensional change of plates made of ledeburitic cold-work tool steels and a working hardness of 61 HRC can be taken from the figure. Typical representatives of the new generation of improved toughness 8-9%Cr-steels show slightly higher growth in dimension than the classical 12%Cr-D2 steel. 

The growth in thickness (in the rolling direction) is always significantly higher than in width, confirming again the generally known behavior. Salt-bath heat treatment results in higher distortion than various vacuum heat treatments with high-pressure gas quenching, but the results indicate that there is also a significant scatter for gas quenching depending on the detailed quenching conditions. 

For more information, click on the link below (subscription required). Then scroll to Figure 12. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

Ipsen USA launches service HUB Model for improved customer support

Ipsen USA, Cherry Valley, Illinois, announced the launch of its new Service HUB model, aimed at enhancing customer support across the United States. The HUB system, developed over the past two years under the leadership of Ipsen Global CEO Geoffrey Somary and currently overseen by Chief Service Officer John Dykstra, is now fully operational across the Midwest and Southeastern regions.

The HUBs are designed to offer quicker response times, with dedicated teams that provide tailored service for customers in close geographic proximity. This model allows Ipsen to optimize service efficiency, reducing downtime for heat-treating operations and improving customer experience.

In addition to benefiting customers, the HUB model also enhances the work-life balance of Ipsen’s Field Service Engineers (FSEs) by reducing travel time. The initiative is led by Lu Chouraki, Manager of Business Development, who emphasized the goal of minimizing response times and improving support for customers facing operational outages.

This strategic shift reflects Ipsen’s commitment to service excellence, offering personalized, regional expertise that both empowers its team and delivers enhanced support to customers.

Read further here. 

Nitrex celebrates 40 Years of innovation in heat treatment solutions

Nitrex, Quebec, announced that it is celebrating its 40th anniversary this year, marking four decades of growth and innovation in the heat treatment industry. Founded in 1984, Nitrex has evolved from a pioneer in controlled nitriding to a global leader offering end-to-end heat treatment solutions. The company’s technological advancements have expanded its capabilities to encompass metallurgy, engineering, process optimization, and automation.

Since 2019, under the current leadership, Nitrex has broadened its portfolio to include advanced vacuum furnaces and introduced technology for improved brake rotor performance. The company has also launched digital platforms such as QMULUS, aimed at optimizing customer processes and boosting operational efficiency.

In addition to its own milestone, Nitrex is celebrating the 50th anniversary of its UPC-Marathon office in Germany, recognizing the long-standing contributions and achievements of its global team. These anniversaries reflect Nitrex’s ongoing commitment to innovation and excellence.

Read further here.

Bodycote presented aerospace materials solutions at Farnborough International Airshow

Bodycote, Macclesfield, U.K., participated in the 2024 Farnborough International Airshow, held this summer.

Bodycote showcased its advanced thermal processing solutions specifically designed for the aerospace industry. The airshow, a key event for aerospace innovation, emphasizes themes like sustainability, future flight, and workforce development, providing Bodycote with a platform to highlight its role in enhancing the performance and reliability of aerospace components.

At the event, visitors could explore Bodycote’s range of services, including heat treatment, metal joining, and specialized thermal processes such as hot isostatic pressing and thermal spray coatings. These processes are essential for improving the properties of metals and alloys in aerospace applications, helping them withstand the stringent requirements of the industry.

Bodycote’s presence at the Farnborough Airshow underscores its expertise and ongoing commitment to fostering collaborations that drive progress in the aerospace, aviation, and defense sectors.

Read further here. 

Dean Schauer appointed chairman of the board at Confluent Medical Technologies

Confluent Medical Technologies, Scottsdale, AZ, announced that Dean Schauer has been appointed Chairman of the Board, effective September 9, 2024.

Schauer, who has served as the company’s CEO for over a decade, will now take on the additional role of Chairman while continuing his responsibilities as CEO and President. Schauer expressed his gratitude for the trust placed in him by investors and employees, stating, “I am honored to guide the company into the next phase as we continue to deliver value to our partners and the patients they serve.”

Under Schauer’s leadership, Confluent has seen significant growth, with revenue more than quadrupling. His appointment aligns with the company’s strategic goals to enhance its materials science capabilities and expand customer partnerships. Earlier this year, Confluent welcomed Sandy Stojkovski and Brian Yoor to the board, further strengthening its leadership team. TPG, a global asset management firm, invested in Confluent in 2022, underscoring confidence in Schauer’s leadership.

Read further here.

Furukawa Electric announces simplified absorption-type split for Optical Fiber and Cable products business

Furukawa Electric Co., Ltd., announced that its Board of Directors has approved a reorganization plan to streamline its optical fiber and cable products business. The company will establish a new wholly-owned subsidiary, referred to as the “New Company,” which will succeed its optical fiber and cable business through an absorption-type split. Additionally, the new company will assume the shares of Shoden Seiwa Co., Ltd., a subsidiary engaged in optical fiber and cable products.

To support this restructuring, Furukawa Electric will create another subsidiary, the “Holding Company,” to manage its global optical fiber operations, including OFS Fitel, LLC in the U.S. and Furukawa Electric LatAm S.A. in Brazil. The reorganization aims to integrate the company’s operations more efficiently on a global scale.

The split, effective April 1, 2025, is intended to strengthen Furukawa’s market position and enhance its ability to respond to evolving industry challenges while maintaining its focus on innovation and operational efficiency.

Read further here

One Minute Mentor: Distortion of High-Speed Steels

High-speed steels show a typical distortion behavior depending on the heat treatment parameters. The figure shows the change in length of cylindrical bars (diameter = 20 mm, or 0.8 in.) and length = 140 mm, or5.5 in.), with rolling direction longitudinal to the sample) for various heat treatment conditions with austenitizing, salt bath quenching, and double tempering.

Quenching and tempering up to 500 °C (930 °F) results only in very small changes in length (either growth or shrinking). Higher tempering temperatures lead to a transformation of the retained austenite into martensite and a corresponding growth in length. For typical tempering temperature of 560 °C (1040 °F) changes in length of about 0.2% take place. Additional alloying with Co (5%) leads to slightly higher changes in length. The effect of an additional third tempering shifts the curve slightly to the left, whereas oil quenching leads to a slight reduction of the change in length.

For more information, click on the link below (subscription required). Then scroll to Figure 9. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

One Minute Mentor: Improving the Homogeneity of the Distortion Behavior

Controlling out-of-roundness is important for certain precision applications, such as class C and D cutting hobs made of high-speed steels. Class C and D hobs must be held close to size limits because they are not ground to size after heat treatment, but rather are used in the unground condition.

Normal size distortion in hardening and tempering can be accommodated by making the tool slightly oversize or slightly undersize, as required, before heat treating. High-speed steel bars, however, have been observed to go out-of-round as much as 0.05 mm (0.002 in.) during heat treatment. The pattern of size distortion shown in Fig. 8 can occur. It appears to be related to the initial shape of the cast ingot and to the specific primary-mill processing used to reduce the ingot into bars.

For more information, click on the link below (subscription required). Then scroll to Figure 8. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

Metex Heat treating announces acquisition of Exactatherm Ltd

Metex Heat Treating, Mississauga, ON, has announced the acquisition of Exactatherm Ltd, a specialist in heat treating for the aerospace, stainless, and tool steels industries. This acquisition is a key part of Metex’s strategy to expand its capabilities and provide comprehensive solutions to clients across the automotive, aerospace, nuclear, commercial, and tool and die sectors.

With this acquisition, Metex will leverage Exactatherm’s industry expertise alongside its own advanced technologies, further strengthening its market position. Exactatherm will continue to operate as a separate entity under the Metex group, maintaining its established reputation for delivering high-quality services.

“This acquisition reinforces our commitment to providing unmatched solutions to our customers,” said Surjit Bawa, President of Metex Heat Treating Ltd. “Together, we will build on our shared strengths and create new opportunities for growth.”

Metex Heat Treating was founded in 1983 and has grown to be the largest heat treater in Canada, specializing in various heat treatment process

Read further here

Ipsen announces launch of field service engineer academy

Ipsen, Cherry Valley, IL, has announced the launch of its Field Service Engineer (FSE) Academy, a 20-week training program aimed at strengthening the Ipsen Customer Service (ICS) Team. The program includes both classroom instruction at the company’s TDC facility in Cherry Valley, Illinois, and hands-on field training with veteran technicians. While primarily designed for new hires, experienced engineers can also participate, with regional service managers directing them to specific modules based on their skill level assessments.

The academy will focus on the fundamentals of vacuum furnace repair, giving technicians a comprehensive understanding of Ipsen’s equipment and customer applications. Technical Training Lead Cavan Cardenas noted, “From day one, we want our technicians to grasp how our products work and their purpose in the field.”

In addition to technical training, the program will develop soft skills and address the demands of a service-driven role, preparing recruits for a dynamic, on-the-road service environment.

Read further here.

Solar Atmospheres announces rapid progress on Michigan facility expansion

Solar Atmospheres, Chesterfield, MI, announced significant progress on the 20,000-square-foot expansion of its Michigan facility. The Delta Industrial team quickly erected the steel structure in just one week. The new expansion will accommodate additional vacuum and air furnaces and provide a dedicated shipping and receiving area. The project remains on schedule for completion by the end of 2024, marking a key step in enhancing Solar Atmospheres’ operational capabilities.

Read further here: 

SECO/WARWICK announces expansion of Meadville facilities

SECO/WARWICK, Meadville, PA, has announced plans to expand its manufacturing facilities to enhance service for North American customers. The expansion involves relocating part of its manufacturing operations and a metallurgical lab for vacuum furnaces from Poland to Crawford County, PA.

Pennsylvania’s Department of Community and Economic Development (DCED) will support this initiative with a $2 million grant under the Redevelopment Assistance Capital Program (RACP), which SECO/WARWICK will match. Additionally, $69,000 in matching funds will be provided for job training through the Workforce & Economic Development Network (WEDnet).

The expansion will occupy a 120,000 sq. ft. facility in the Crawford Business Park, a site redeveloped from the former American Viscose Corporation mill. This development is expected to benefit the community and bolster SECO/WARWICK’s capabilities in producing heat-treating and aluminum melting furnaces.

Read further here