One Minute Mentor: Equipment for Forging

The forge quenching process requires that quenching equipment be placed as closely as possible to the equipment used in the forging stage. Since the early 1960s, various direct-forge and quench equipment has been installed in this manner, thus enabling the use of carbon steels, which have good hardenability from grain growth and high dislocation density from the thermomechanical deformation performed during hot forging.

Continue reading

Constellium developing aluminum-lithium alloys for NASA

Constellium, Paris, is developing an aluminum-lithium alloy solution, Airware®, that will be used for NASA’s Launch System rocket and Orion spacecraft, for missions that will ultimately send humans farther into deep space than ever before. Airware’s inherent low density, high-specific stiffness, strength and excellent mechanical properties provide the high-performance characteristics required during the demanding launch and landing phases.

Continue reading

Spray Tips: Motion control

Although handheld spraying has been carried out for nearly a century, it is not the preferred or safest means of spraying; motion control is necessary to ensure operator safety and coating quality.

Continue reading

EHLA Tuning: roller coating at up to 200 meters per minute

Scientists at the Fraunhofer Institute for Laser Technology (ILT), Germany, together with three industrial partners, have developed high-speed laser material deposition process parameters and strategies for coating and repair as well as for hybrid manufacturing of sealing surfaces in its collaborative project EVEREST.

Continue reading

Battelle awarded contract to support manufacturing of materials for extreme hypersonic environments

Battelle has won a potential seven-year, $46.3 million contract to help the Department of Defense support the manufacture of thermal protection materials that can withstand extreme hypersonic environments. The Manufacturing of Carbon-Carbon Composites for Hypersonic Applications initiative seeks to rapidly mature and integrate manufacturing innovations that will accelerate the production of carbon-carbon composites.

Continue reading