Improving steelmaking with industrial gas technologies

Experts in steel metallurgy and process gas engineering from Linde LLC and Linde Engineering North America Inc. are showcasing technologies for improving plant productivity, product quality and environmental performance at AISTech 2015 at the Cleveland Convention Center, May 4-7.

Continue reading

Electron spin brings order to high entropy alloys

Researchers from North Carolina State University, Raleigh, discovered that electron spin brings a previously unknown degree of order to the high entropy alloy nickel iron chromium cobalt (NiFeCrCo)— and may play a role in giving the alloy its desirable properties.