Surprising discovery of grain boundary structures

Scientists from the Research Center Future Energy Materials and Systems of the University Alliance Ruhr, Germany, used state-of-the-art microscopy and simulation techniques to systematically observe how iron atoms alter the structure of grain boundaries in titanium. They were surprised by the results: “Iron atoms not only segregate to the interface, but they form entirely unexpected cage-like structures,” explains Prof. Christian Liebscher, lead of the international research team. The researchers did not expect such a behavior.

Continue reading

Nikon divests laser scanning division in agreement with UK’s Metrology

Nikon Corp. (Tokyo) has announced that U.K.-based LK Metrology Ltd. (Derby) has acquired Nikon’s laser scanning and Focus Inspection software business. The acquisition makes strategic sense, as the two companies have previously worked together providing non-contact inspection solutions. In addition, Nikon’s deal with long-time collaborator LK Metrology, ensures continued development of its pioneering 3D measurement technology.

Continue reading

ORNL research aims to support production of large-scale components

Researchers at the US Department of Energy’s Oak Ridge National Laboratory (ORNL) in Tennessee are leveraging advanced manufacturing techniques, such as Hot Isostatic Pressing (HIP) Powder Metallurgy and Additive Manufacturing, to produce parts weighing over 4,500 kg. ORNL highlights the urgent need for these large-scale components across various sectors, including aerospace, defense, nuclear, oil, gas, renewables, and construction. This demand is particularly pressing in the US, where traditional manufacturing methods like casting and forging have declined and moved overseas, leading to supply-chain shortages.

Senior research scientists Jason Mayeur and Soumya Nag are hoping to add Wire Arc Additive Manufacturing (WAAM), hybrid manufacturing, in-situ monitoring and advanced computational modeling to HIP technology to create molds faster and more accurately whilst leveraging the PM technology American manufacturers may be more acquainted with.

“PM-HIP is a vital pathway for diversifying the supply chain for producing large-scale metal parts that are becoming more difficult to source via conventional means,” Mayeur explained. “The technology is of particular interest to the nuclear and hydroelectric industrial sectors, as well as the Department of Defense.”

In contrast with traditional casting and forging techniques, PM-HIP involves fabricating pre-formed, hollow molds for each large-scale component and filling them with metal powder. Once the additively manufactured mold (aka a ‘can’ or ‘capsule’) receives an initial seal, any gas remaining inside is pumped out. Then, a more permanent hermetic seal is applied.

At this point, the capsule is heated and pressurized in prescribed cycles within a Hot Isostatic Press (essentially a pressurized furnace). Without melting, these cycles facilitate the consolidation of the metal powder into the required shape in a process exchange of heat and pressure known as solid-state bonding. When bonding is complete, acid leaching or machining is used to remove the exterior can, revealing the intended part.

Jason Mayeur works in the Deposition Science and Technology Group at ORNL, where he applies his knowledge in computational solid mechanics to manufacturing challenges. His two-decade research career began with the use of computational models to understand the relationships between materials microstructure and performance. He has since segued into the analysis of the structural material performance of metals and alloys.

In this arena, Mayeur develops theory, writes code to implement his theories, and then performs simulations of solids under various loading conditions to determine their suitability for use in a variety of applications. In short, Mayeur’s code can be used to improve the PM-HIP process, thus making it a more attractive alternative to traditional casting and forging.

Soumya Nag, Mayeur’s colleague at ORNL, works in the Materials Science and Technology Division, applying his own two decades of research experience in materials and manufacturing. Nag is a metallurgist with expertise in evaluating lightweight, high-temperature structural alloys fabricated via conventional and advanced manufacturing techniques.

“Jason is an expert in predictive modeling of deformation characteristics of Hot Isostatic Pressing canisters. I am more involved in the experimental side of things. Jason and I complement each other, and really, our two efforts are very much intertwined and critical toward the overall success of the task,” Nag said.

Nag’s research centers on the processing and materials science of HIP capsule fabrication, using various additive manufacturing techniques and assessing the quality of the resulting component parts.

“Additive Manufacturing offers unique design flexibility, which, combined with the reliability of PM-HIP, can pave the path toward precise manufacturing of large-scale, custom and complex, energy-related parts while also taking advantage of multi-material builds,” he explained.

Nag collaborates with Mayeur to design and perform experiments that characterize the metal powder material’s behavior and its mechanical properties in pursuit of a better, more accurate build while providing the necessary material property inputs for Mayeur’s computational models.

Mayeur’s work targets many technological challenges posed by the PM-HIP process, striving for quality and consistency in geometry to achieve dimensional accuracy at a very large scale. One challenge is shrinkage. During PM-HIP, the volume of metal powder within the can shrinks by approximately 30%, but not uniformly.

To address these inconsistencies, Mayeur’s computational models work to predict how the shrinkage occurs for different part geometries and capsule designs. This is an iterative process that occurs after initial capsule design, using the simulation results as a guide to modify the final design.

For more information: Oak Ridge National Laboratory (ORNL)

Image: This additively manufactured PM-HIP will be used to create an impeller for a hydropower impeller, demonstrating a new approach for creating large-scale clean energy components. (Courtesy Carlos Jones/ORNL, US DoE)

University of Illinois Chicago students write the book on automating diamond membrane creation for quantum devices

Six undergraduates at the University of Illinois Chicago (UIC) have been developing a process to accelerate the creation of diamond membranes, which are crucial for hosting qubits, the fundamental units of quantum information. This work is part of the research at Q-NEXT, a U.S. Department of Energy National Quantum Information Science Research Center led by Argonne National Laboratory. During their 10-week internship at Argonne, the students wrote software to automate a labor-intensive part of diamond-membrane production, finding the experience both challenging and rewarding.

Their work is enabled through Break Through Tech Chicago, an initiative that provides women and nonbinary people with internship opportunities in science and technology. Argonne staff scientist Nazar Delegan, a Q-NEXT collaborator, and UIC professor Dale Reed led the student team.

Quantum information technologies are expected to revolutionize areas such as logistics, drug development and navigation in the coming decades. Diamond membranes are a new material for hosting qubits, the core of quantum devices. The membranes have desirable properties for quantum information processing, and they open paths for integrating quantum materials with current information technologies.

Scientists are investigating the most effective ways to fabricate diamond membranes. One of the production steps — a specific process in the etching stage — requires up to 60 minutes of continual human effort and supervision.

The task before the UIC students: Put that etching process on the path to full automation.

“There are factors that can disrupt the etching process. Someone has to constantly be checking that it’s being done right,” said Fernanda Villalpando, an information decision sciences senior and the group’s project manager. ​“So we worked to automate it.”

By demonstrating proof of concept, the students laid the groundwork for the procedure so that future researchers can scale it up to industry production levels.

The membranes are created by embedding a layer of graphite between two layers of diamond. The thick bottom diamond layer serves as a platform. The tissue-thin top layer — 100 to 1,000 nanometers thin, a hundred to a thousand times thinner than a sheet of paper — is the diamond membrane. Scientists use electrical probes to chemically etch away the graphite beneath the membrane, which can then be peeled off and integrated into a quantum device.

Currently, a human must watch over the roughly hour-long etching process to ensure its successful execution. But following the UIC group’s work, researchers will one day be able to say goodbye to human-supervised etching.

Building on image detection software called Open CV as part of the Python programming language, the students created a program to teach the computer to visually assess and respond to the etching process. Is there a bubble trapped between layers? An unexpected obstruction? With the UIC group’s program, the computer knows whether to stop the etch, continue or work around it.

“That way, the scientists don’t have to be there to push the ​‘off’ button, for example,” Villalpando said. ​“Our program stops it for them.”

As the ones spearheading the procedure, the team had no blueprint for how to proceed. They quickly realized they’d have to draw heavily on their computer science knowledge, hunt for relevant documentation and even pick up the phone to call the device’s manufacturer for minutiae not captured in the literature.

“We had to reach out to the company. It was a little frustrating, because how were we going to do the rest of the work if we’re having trouble communicating with the devices?” said Claudia Jimenez, a computer science junior. ​“But once we got that part, we had the persistence and resilience to keep going, and made a lot of progress in two or three weeks. We kept going and looked for different resources to accomplish something that none of us had ever done before.”

In fact, it was something no one had done before. Currently, only a select few groups in the world are creating diamond-membrane qubit platforms.

“I love being in a space where everyone is excited about it,” Villalpando said. ​“I’ve been in rooms where people do the work that they do all the time. It’s not new, and there’s only one way to do it. But we get to be creative and think, ​‘How can we solve this?’”

For Q-NEXT, the group’s development of a technical procedure from scratch was a crucial contribution to quantum materials fabrication. For the students, it was part of the real-world work of experimenting in a laboratory.

The Chicago Quantum Exchange honored the group’s work with the Best Undergraduate Student Poster Award at the Chicago Quantum Summit in October.

The UIC team was also excited to be part of game-changing research that could have impacts across so many areas of everyday life.

“Quantum applies to so many different applications and fields and industries. I would possibly like to be a part of that. It was nice to hear from actual professionals in the field giving an explanation about what quantum is, how it can be applied and how we’re actually going to do it,” Jimenez said.

For more information: Q-NEXT

Image: UIC students work at the Argonne Quantum Foundry through the Break Through Tech Chicago program, helping automate an important step in the production of diamond membranes for qubits. (Image by Argonne National Laboratory.)

Deep learning streamlines identification of 2D materials

Researchers have developed a deep learning-based method that enhances the speed and accuracy of identifying and classifying two-dimensional (2D) materials using Raman spectroscopy. Traditional Raman analysis is slow and requires manual interpretation, but this new approach accelerates the development and analysis of 2D materials, which are crucial for electronics and medical technologies. Lead researcher Yaping Qi from Tohoku University explains that their generative model improves limited and unevenly distributed spectral data, effectively filling in the gaps.

The learning model used spectral data from seven different 2D materials and three distinct stacked combinations. The researchers introduced an innovative data augmentation framework using Denoising Diffusion Probabilistic Models (DDPM) to generate additional synthetic data and address these challenges. For this type of model, noise is added to the original data to enhance the dataset, and then the model learns to work backward and remove this noise to generate a novel output that is consistent with the original data distribution.
By pairing this augmented dataset with a four-layer Convolutional Neural Network (CNN), the research team achieved a classification accuracy of 98.8% on the original dataset and, notably, 100% accuracy with the augmented data. This automated approach not only enhances classification performance but also reduces the need for manual intervention, improving the efficiency and scalability of Raman spectroscopy for 2D material identification.

“This method provides a robust and automated solution for high-precision analysis of 2D materials,” summarizes Qi, “The integration of deep learning techniques holds significant promise for materials science research and industrial quality control, where reliable and rapid identification is critical.”

The study presents the first application of DDPM in Raman spectral data generation, paving the way for more efficient, automated spectroscopy analysis. This approach enables precise material characterization even when experimental data is scarce or difficult to obtain. Ultimately, this can allow for research done in the lab to transform into a real product that consumers can buy in stores into a much smoother process.

For more information: Tohoku University

Invisible touch: Stevens is giving AI the ability to feel and measure surfaces

AI technologies have advanced in seeing, conversing, calculating, and creating, but they have struggled to measure or “feel” surfaces. According to Stevens physics professor Yong Meng Sua, while AI has developed a sense of sight, it hasn’t yet achieved a human-like sense of touch to distinguish textures. However, researchers at Stevens’ Center for Quantum Science and Engineering (CQSE) have now demonstrated a method to give AI the ability to feel.

Sua, working with CQSE Director Yuping Huang and doctoral candidates Daniel Tafone and Luke McEvoy ’22 M.S. ‘23, devised a quantum-lab setup that combines a photon-firing scanning laser with new algorithmic AI models trained to tell the differences among various surfaces as they are imaged with those lasers.

In their system, a specially created beam of light is pulsed in short blasts at a surface to “feel” it. Reflected, back-scattered photons return from the target object carrying speckle noise, a random type of flaw that occurs in imagery.

Speckle noise is normally considered detrimental to clear, accurate imaging. However, the Stevens group’s system takes a different approach: it detects and processes these noise artifacts using an AI that has been carefully trained to interpret their characteristics as valuable data. This allows the system to accurately discern the topography of the object.

“We use the variation in photon counts over different illumination points across the surface,” says Tafone.

The team used 31 industrial sandpapers with surfaces of varying roughness, ranging from 1 to 100 microns thick, as experimental targets. (For comparison, an average human hair is about 100 microns thick.) Mode-locked lasers generated light pulses aimed at the samples.

Those pulses passed through transceivers, encountered the sandpapers, and then rebounded back through the system for analysis by the team’s learning model.

During early tests, the group’s method averaged a root-mean-square error (RMSE) of about 8 microns; after working with multiple samples and averaging results across them, its accuracy improved significantly to within 4 microns, comparable to the best industrial profilometer devices currently used.

“Interestingly, our system worked best for the finest-grained surfaces, such as diamond lapping film and aluminum oxide,” notes Tafone.

The new method could be useful for various applications, he adds.

For example, human examiners often make mistakes when attempting to detect skin cancers, confusing very similar-looking but harmless conditions with potentially fatal melanomas.

“Tiny differences in mole roughness, too small to see with the human eye but measurable with our proposed quantum system, could differentiate between those conditions,” explains Huang. “Quantum interactions provide a wealth of information, using AI to quickly understand and process it is the next logical step.”

Manufacturing quality control of components, as well, often hinges on extremely small distances that can mean the difference between a perfect part and a tiny defect that could eventually cause a dangerous mechanical failure.

“Since LiDAR technology is already implemented widely in devices such as autonomous cars, smartphones and robots,” Huang concludes, “our method enriches their capabilities with surface property measurement at very small scales.”

For more information: Applied Optics

NIST Seeks Critical and Emerging Technology Information

The National Institute of Standards and Technology (NIST) is requesting information related to the Implementation Roadmap for the U.S. Government National Standards Strategy for Critical and Emerging Technology.

In this Request for Information (RFI), NIST is seeking information about the following topics:

  • Existing awards and recognition programs that the U.S. government and U.S. standards community can use to encourage and support participation and leadership in standards development for critical and emerging technologies.
  • Ways the U.S. government and the U.S. standards community can educate and empower the standards workforce and business and technology decision-makers.
  • Feedback on how NIST can best maintain an open dialogue and sustained communication with the U.S. critical and emerging technologies and standards communities regarding the ongoing implementation of the roadmap.

The U.S. Government National Standards Strategy for Critical and Emerging Technology promotes technologically sound standards that help American industry compete internationally on a level playing field. It is intended to support and complement existing private sector-led standards activities.

For more information: Federal Register

New Automatic and Manual High Pressure Ceramic Shell Removal Center

Franklin Precision Castings announced the acquisition of a state-of-the-art 20,000 PSI water blasting system, combining both automatic and manual operations for ceramic shell removal. This cutting-edge technology from Triplex Systems, Inc. of Minnesota, marks a continued advancement in its commitment to quality, efficiency, and workplace safety.

“The Triplex water blasting system has reduced our cycle times by 50 to 75%, a remarkable improvement,” said Mark Johnson, Cleaning Room Supervisor at Franklin Precision Castings.

The new high-pressure water jet blasting machine allows for safer and more efficient ceramic shell removal, improved consistency in part processing, and shorter cycle time, allowing our customers to get parts even faster. In addition to boosting efficiency, the system reduces water consumption by 50%. The built-in drag conveyor unloads broken ceramic shell into a hopper, mitigating the risk of back injuries and enhancing overall safety in our operations.

The Model TRX-1250CAM combines the power of automatic and manual cleaning cycles within a single cabinet. This innovative technology allows operators to seamlessly switch between modes via a user-friendly touch-screen interface, all powered by a single high-pressure pump unit.

This investment reinforces Franklin Precision Castings’ ongoing commitment to continuous improvement.

For more information: Franklin Castings

New Machine Learning Model Predicts Dielectric Function of Materials

Cutting-edge researchers Tomohito Amano and Shinji Tsuneyuki at the University of Tokyo, alongside Tamio Yamazaki from CURIE, have unveiled a machine learning model that revolutionizes our approach to predicting the dielectric function of materials – moving beyond traditional first-principles calculations.

This critical function gauges the polarization of negative and positive charges within materials, forming the core concept behind dielectric materials.

With this innovative model, scientists can achieve rapid and precise predictions of dielectric functions, paving the way for the creation of next-generation dielectric materials essential for transformative technologies, including the anticipated advancements in 6G network.

While not as widely recognized as semiconductors, dielectric materials hold immense promise for enhancing modern electronic systems. These materials offer a unique characteristic: they do not conduct electricity well but are not insulators either. When subjected to an electric field, positive charges within the material are drawn toward the field, while negative charges shift in the opposite direction, leading to dielectric polarization.

This polarization is quantified by the dielectric function, a critical measure of its strength. Despite its significance, calculating the dielectric function generally requires complex first-principles approaches rooted in quantum mechanics, making it a time-consuming and resource-intensive endeavor.

Researchers have successfully developed an innovative machine-learning model designed to tackle significant challenges in materials science. They’ve taken a groundbreaking approach by generating training data through first-principle calculations of the electronic states of various materials.

Instead of relying on conventional calculations focused on individual molecules, this model emphasizes the chemical bonds between atoms. Its accuracy was rigorously tested against empirical data from simple molecules like methanol and ethanol.

This model not only describes the electronic states of a variety of materials with nearly the same accuracy as traditional methods but also does so while dramatically reducing computational demands. Its capability for large-scale and long-term simulations opens new doors, enabling researchers to investigate the macroscopic origins of dielectric properties in complex molecular systems—a feat previously hindered by computational costs.

Despite these impressive achievements, scientists are already envisioning future possibilities.

For more information: Physical Review B

Developing New High-Performance and Recyclable Materials

Professor Chiyoung Park of the Department of Energy Science and Engineering at DGIST has developed a groundbreaking new material poised to advance high-sensitivity recyclable sensor technology. Working in collaboration with Professor U-hyeok Choi of Inha University, Park’s team created a recyclable high-sensitivity sensor based on the dynamic polymer network. This next-generation material is garnering attention for its ability to combine environmental sustainability with high performance.

Existing high-sensitivity sensors have been limited by performance degradation due to fatigue and repeated use.

However, the dynamic polymer network developed by the research team maintains excellent sensitivity and durability by using vinylogous urethane bonding.

This bonding structure self-heals in response to external stimuli such as temperature, light, and pressure, preventing performance degradation even after repeated use.

The dynamic polymer network is also sensitive to various mechanical movements, heat, and light, and sensors based on the network excel at detecting human body movements.

Researchers have demonstrated that the sensors can accurately detect finger bends, changes in facial expressions, and even swallowing movements in the throat.

One of the biggest strengths of the technology is that it can maintain the same sensitivity after recycling without any degradation.

Addressing the growing issue of e-waste, the team designed the technology to combine recyclability with high performance.

They believe the dynamic polymer network’s versatility supports repeated use and recycling, potentially leading to significant reductions in e-waste.

Their work promises to have far-reaching implications not only in sensor technology but also in next-generation electronics, wearable devices, and medical equipment.

The team continues to work on commercializing the technology for widespread industrial applications.

“Our material offers excellent processability and can be recycled mechanically or chemically,” said DGIST Professor Chiyoung Park.

“The polymer network undergoes a simple recycling process, which we expect will extend the lifespan of electronic devices and wearable sensors, significantly reducing electronic waste.”

For more information: Chemical Engineering Journal

New insights into uranium’s tricky chemistry

Uranium is known as the heavy metal with an intricate chemistry and diverse bonding behaviors, as well as being radioactive. Now, an international team of scientists have utilized synchrotron light at the Rossendorf Beamline (ROBL) to explore the unique properties of low-valent uranium compounds. At the European Synchrotron Radiation Facility (ESRF) in Grenoble, France, the Helmholtz-Zentrum Dresden-Rossendorf (HZDR) runs four experimental stations for radiochemical experiments.

Continue reading

Scanbot streamlines materials research with STM automation

Researchers at Monash University (Melbourne, Australia) developed a new open-source software package that aims to significantly streamline the study of materials using scanning tunneling microscopes (STMs). The software, named Scanbot, automates the time-consuming probe optimization and data acquisition processes essential for STM experiments, helping to accelerate 2D materials research by enabling detailed investigation after the STM tip has been automatically optimized and sharpened.

Continue reading

Engineering perovskite materials at the atomic level paves way for new lasers, LEDs

Researchers have developed a technique to engineer layered hybrid perovskites (LHPs) down to the atomic level, precisely controlling how these materials convert electrical charge into light. This advancement paves the way for creating materials tailored for next-generation printed LEDs and lasers, and holds promise for engineering other materials for photovoltaic devices.

Perovskites, known for their crystalline structure, possess desirable optical, electronic, and quantum properties. LHPs are composed of thin sheets of perovskite semiconductor material separated by organic spacer layers, which can be laid down as thin films. These materials are highly efficient at converting electrical charge into light, making them ideal for use in next-generation LEDs, lasers, and photonic integrated circuits. Despite their potential, understanding how to engineer LHPs to control their performance characteristics has been a challenge for researchers until now.

To understand what the researchers discovered, you have to start with quantum wells, which are sheets of semiconductor material sandwiched between spacer layers.

“We knew quantum wells were forming in LHPs – they’re the layers,” says Aram Amassian, corresponding author of a paper on the work and a professor of materials science and engineering at North Carolina State University.

And understanding the size distribution of quantum wells is important because energy flows from high-energy structures to low-energy structures at the molecular level.

“A quantum well that is two atoms thick has higher energy than a quantum well that is five atoms thick,” says Kenan Gundogdu, co-author of the paper and a professor of physics at NC State. “And in order to get energy to flow efficiently, you want to have quantum wells that are three and four atoms thick between the quantum wells that are two and five atoms thick. You basically want to have a gradual slope that the energy can cascade down.”

“But people studying LHPs kept running into an anomaly: the size distribution of quantum wells in an LHP sample that could be detected via X-ray diffraction would be different than the size distribution of quantum wells that could be detected using optical spectroscopy,” Amassian says.

“For example, diffraction might tell you that your quantum wells are two atoms thick, as well as there being a three-dimensional bulk crystal,” Amassian says. “But spectroscopy might tell you that you have quantum wells that are two atoms, three atoms, and four atoms thick, as well as the 3D bulk phase.

“So, the first question we had was: why are we seeing this fundamental disconnect between X-ray diffraction and optical spectroscopy? And our second question was: how can we control the size and distribution of quantum wells in LHPs?”

Through a series of experiments the researchers discovered that there was a key player involved in answering both questions: nanoplatelets.

“Nanoplatelets are individual sheets of the perovskite material that form on the surface of the solution we use to create LHPs,” Amassian says. “We found that these nanoplatelets essentially serve as templates for layered materials that form under them. So, if the nanoplatelet is two atoms thick, the LHP beneath it forms as a series of two-atom-thick quantum wells.

“However, the nanoplatelets themselves aren’t stable, like the rest of the LHP material. Instead, the thickness of nanoplatelets keeps growing, adding new layers of atoms over time. So, when the nanoplatelet is three atoms thick, it forms three-atom quantum wells, and so on. And, eventually, the nanoplatelet grows so thick that it becomes a three-dimensional crystal.”

This finding also resolved the longstanding anomaly about why X-ray diffraction and optical spectroscopy were providing different results. Diffraction detects the stacking of sheets and therefore does not detect nanoplatelets, whereas optical spectroscopy detects isolated sheets.

“What’s exciting is that we found we can essentially stop the growth of nanoplatelets in a controlled way, essentially tuning the size and distribution of quantum wells in LHP films,” Amassian says. “And by controlling the size and arrangement of the quantum wells, we can achieve excellent energy cascades – which means the material is highly efficient and fast at funneling charges and energy for the purposes of laser and LED applications.”

When the researchers found that nanoplatelets played such a critical role in the formation of perovskite layers in LHPs, they decided to see if nanoplatelets could be used to engineer the structure and properties of other perovskite materials – such as the perovskites used to convert light into electricity in solar cells and other photovoltaic technologies.

“We found that the nanoplatelets play a similar role in other perovskite materials and can be used to engineer those materials to enhance the desired structure, improving their photovoltaic performance and stability,” says Milad Abolhasani, co-author of the paper and ALCOA Professor of Chemical and Biomolecular Engineering at NC State.

For more information: Matter

New technology improves structural strength

Researchers from Texas A&M University and Sandia National Laboratories have significantly enhanced interlocking metasurfaces (ILMs) using shape memory alloys (SMAs), offering a stronger and more stable alternative to traditional joining techniques like bolts and adhesives, with potential applications in aerospace, robotics, and biomedical devices.

“ILMs are poised to redefine joining technologies across a range of applications, much like Velcro did decades ago,” said Dr. Ibrahim Karaman, professor and head of the Department of Materials Science and Engineering Department at Texas A&M. “In collaboration with Sandia National Laboratories, the original developers of ILMs, we have engineered and fabricated ILMs from shape memory alloys. Our research demonstrates that these ILMs can be selectively disengaged and re-engaged on demand while maintaining consistent joint strength and structural integrity.”

Similar to Legos or Velcro, ILMs enable the joining of two bodies by transmitting force and constraining movement. Until now, this joining method has been passive, requiring force for engagement.

Control of joining technology through temperature changes opens new possibilities for smart, adaptive structures without loss in strength or stability and with increased options for flexibility and functionality.

“Active ILMs have the potential to revolutionize mechanical joint design in industries requiring precise, repeatable assembly and disassembly,” said Abdelrahman Elsayed, graduate research assistant in the materials science and engineering department at Texas A&M.

Practical applications include designing reconfigurable aerospace engineering components where parts must be assembled and disassembled multiple times. Active ILMs could also provide flexible and adaptable joints for robotics-enhancing functionality. In biomedical devices, the ability to adjust implants and prosthetics to body movements and temperatures could offer a better option for patients.

The current findings utilized the shape memory effect of SMAs to recover the ILMs’ shape by adding heat. The researchers hope to build on these findings by using the superelasticity effect of SMAs to create ILMs that can withstand large deformation and instantaneously recover under very high-stress levels.

“We anticipate that incorporating SMAs into ILMs will unlock numerous future applications, though several challenges remain,” said Karaman. “Achieving superelasticity in complex 3D-printed ILMs will enable localized control of structural stiffness and facilitate reattachment with high locking forces. Additionally, we expect this technology to address longstanding challenges associated with joining techniques in extreme environments. We are highly enthusiastic about the transformative potential of ILM technology.”

For more information: Materials & Design

Image: Two proposed versions of ILMs in their different engagement states.

Novel technique for observing atomic-level changes could unlock potential of quantum materials

A research team from the Department of Energy’s Oak Ridge National Laboratory has developed the Rapid Object Detection and Action System (RODAS), a unique method that combines imaging, spectroscopy, and microscopy to observe changes in materials at the atomic level. This technique offers new opportunities for understanding and developing advanced materials for quantum computing and electronics by capturing the properties of fleeting atomic structures as they form, providing unprecedented insights into the evolution of material properties at the smallest scales.

Traditional approaches combining scanning transmission electron microscopy, or STEM, with electron energy loss spectroscopy, or EELS, have been limited because the electron beam can change or degrade the materials being analyzed. That dynamic often causes scientists to measure altered states rather than the intended material properties. RODAS overcomes the limitation and also integrates the system with dynamic computer-vision-enabled imaging, which uses real-time machine learning.

When analyzing the specimen, RODAS focuses only on areas of interest. This approach enables rapid analysis—in seconds or milliseconds—compared with sometimes several minutes that can be required by other STEM-EELS methods. Importantly, RODAS extracts crucial information without destroying the sample.

All materials have defects, and these defects can directly influence virtually any of a material’s properties—whether electronic, mechanical or quantum, for example. Defects can arrange themselves in a variety of ways at the atomic level, both intrinsically and in response to external stimuli, such as electron beam irradiation.

Unfortunately, the local properties of these various defect configurations are not well understood. Although STEM methods can experimentally measure such configurations, investigating specific configurations without altering them is extremely challenging.

“Understanding defect configurations is crucial for developing next-generation materials,” said the study’s lead author, Kevin Roccapriore of ORNL’s Center for Nanophase Materials Sciences. “If empowered with that knowledge, we could intentionally create a specific configuration to produce a specific property. Such work is entirely separate from the observation and analysis activity but represents one potentially impactful direction for the future.”

The research team demonstrated their technique on single-layer molybdenum disulfide, a promising semiconductor material for quantum computing and optics applications. Molybdenum disulfide is particularly interesting because it can emit single photons from defects known as single sulfur vacancies.

In this material, a single sulfur vacancy refers to the absence of one sulfur atom from its honeycombed lattice structure, which is the arrangement of the atoms. These vacancies can aggregate, creating unique electronic properties that make molybdenum disulfide valuable for advanced technological applications.

By studying molybdenum disulfide and similar single-layer materials, scientists hope to answer vital questions about optical or electronic properties at the atomic scale.

The RODAS technique represents a significant leap forward in materials characterization. It empowers researchers to dynamically explore structure-property relationships during analysis, target specific atoms or defects for measurement as they form, efficiently collect data on various defect types, adapt to identify new atomic or defect classes in real time and minimize sample damage while maintaining detailed analysis.

By applying this technology to a single layer of vanadium-doped molybdenum disulfide, the research team gained new understanding of defect formation and evolution under electron beam exposure. This approach allows for exploring and characterizing materials in dynamic states, offering a deeper knowledge of how materials behave under various stimuli.

“Materials science techniques such as advanced electron microscopy continue to expand our comprehension of the physical world, and systems such as RODAS could play a crucial role in accelerating discovery and innovation,” Roccapriore said.

“The ability to observe and analyze materials at the atomic scale in real time shows potential for pushing the boundaries in computing, electronics and beyond, and ultimately enabling the development of transformative technologies.”

For more information: Science Advances

Image: Electron microscopy measurements are usually performed by collecting all points in a 2D grid. Here, using deep learning in real time, only sites of interest are measured (colored circles), allowing experiments to be conducted on a much larger variety of materials, even those that change under the beam. 

New soft material charges like batteries, can be woven into fabrics, make devices

Scientists from Northwestern University have developed highly energy-efficient, biocompatible materials made of tiny, flexible nano-sized ribbons that can be charged like a battery to store energy or record digital information. These sustainable materials could lead to new types of ultralight electronic devices, reducing the environmental impact of electronic manufacturing and disposal. The study highlights potential applications for these soft materials in low-power, energy-efficient microscopic memory chips, sensors, and energy storage units

Researchers maintain that these materials could also be integrated into woven fibers to create smart fabrics or sticker-like medical implants. In today’s wearable devices, electronics are clunkily strapped to the body with a wristband. But, with the new materials, the wristband itself could have electronic activity.

Northwestern’s Samuel I. Stupp, who led the study, stated that this is a wholly new concept in materials science and soft materials research.
Stupp maintained that researchers imagine a future where you could wear a shirt with air conditioning built into it or rely on soft bioactive implants that feel like tissues and are activated wirelessly to improve heart or brain function.

“Those uses require electrical and biological signals, but we cannot build those applications with classic electroactive materials. It’s not practical to put hard materials into our organs or in shirts that people can wear. We need to bring electrical signals into the world of soft materials. That is exactly what we have done in this study,” added Stupp.

Researchers maintained that the secret behind the new material is peptide amphiphiles, a versatile platform of molecules previously developed in Stupp’s laboratory. These self-assembling structures form filaments in water and have already demonstrated promise in regenerative medicine. The molecules contain peptides and a lipid segment, which drives the molecular self-assembly when placed in water.

In the study, the team replaced the lipid tail with a miniature molecular segment of a plastic called polyvinylidene fluoride (PVDF). But they kept the peptide segment, which contains sequences of amino acids. Commonly used in audio and sonar technologies, PVDF is a plastic with unusual electrical properties.

It can generate electrical signals when pressed or squeezed — a property known as piezoelectricity. It also is a ferroelectric material, which means it has a polar structure that can switch orientation by 180 degrees using an external voltage. The dominant ferroelectrics in technology are hard materials and often include rare or toxic metals, such as lead and niobium.

Stupp stated that PVDF was discovered in the late 1960s and is the first known plastic with ferroelectric properties.

“It has all the robustness of plastic while being useful for electrical devices. That makes it a very high-value material for advanced technologies. However, in pure form, its ferroelectric character is not stable, and, if heated above the so-called Curie temperature, it loses its polarity irreversibly,” said Stupp.

All plastics, including PVDF, contain polymers, which are giant molecules typically composed of thousands of chemical structural units. In the new study, the Stupp laboratory precisely synthesized miniature polymers with only 3 to 7 vinylidene fluoride units. Interestingly, the miniature segments with 4, 5 or 6 units are programmed by nature’s beta-sheet structures, which are present in proteins, to organize into a stable ferroelectric phase, according to the study.

For more information: Nature

Image: This illustration shows a future vision of assemblies of molecules formed by peptides and miniature molecular segments from a plastic material to create ferroelectric structures that switch polarity to store digital information or signal neurons.

Materials Analysis Technology releases a MOU with SGS

Materials Analysis Technology Inc., Taiwan, and Swiss SGS Taiwan Ltd. signed a memorandum of understanding with the goal of providing comprehensive ISO 26262 functional safety product certification services, AEC-Q automotive electronic component reliability verification services, and soft error rate assessment and analysis in the automotive semiconductor and electronic component industries in Taiwan.

Continue reading

Faraday enhances 3D-IC design service with Ansys multiphysics analysis

Faraday Technology Corporation, Pittsburgh, Pa., a leading application specific integrated circuits (ASIC) design service and IP provider, is expanding its use of Ansys technology to enhance its capabilities in developing advanced designs for multi-die 2.5D/3D-ICs — critical for artificial intelligence (AI), IoT, and 5G applications. With support from Ansys, Faraday will empower its customers to explore more robust design options for more innovative products.

Faraday recently announced a 2.5D/3D-IC advanced package service to address exploding demand for multi-die designs that target products with better performance and lower power consumption. To meet this demand, engineers need the right multiphysics analysis tools to verify that chip designs include reliable signal and structural integrity and reliable power distribution before it goes to fabrication. This challenge is compounded by the trend toward developing denser chips that are more vulnerable to EM issues.

Adding RaptorX into the design flow will enable Faraday to increase precision and efficiency in its development process. Moreover, it enables predictively accurate EM modeling and analysis for advanced 3D-IC products, ensuring data transfer meets stringent modern standards. This will improve the design’s fidelity, enhance performance and reliability, and accelerate time-to-market.

“Our extensive silicon IP allows our customers to start designing from a solid foundation, enabling them to focus solely on innovation and differentiating themselves in the market,” said C.H. Chien, vice president of R&D at Faraday. “Fabrication is exceptionally expensive and there is no room for error. So, keeping the overall project cost low is paramount, and it starts with the initial design. With the addition of RaptorX in this phase, we can offer customers an efficient workflow that includes design verification and signoff as well as access to top-tier test and fabrication services, removing doubts about the chip’s performance and longevity.”

“Ansys’ focus on multiphysics platforms enables innovators like Faraday to address key challenges for 3D-IC and accelerate their time-to-market,” said John Lee, vice president and general manager of the semiconductor, electronics, and optics business unit at Ansys. “Our industry-leading tools facilitate meticulous modeling and analysis of electromagnetic phenomena, helping our customers remain at the forefront of technological advancements in 5G, AI, and IoT.”

 

Image – EMag extraction of an interposer lane, including 48 signals in the presence of their respective VDD/VSS network and indicative simulation results, and S-Parameter analysis and transient (eye diagram) analysis of a signal line.

 

For more information:

Ansys

https://www.ansys.com

Faraday Technology Corporation

http://www.faraday-tech.com/

 

 

There’s two sides to this semiconductor, and many simultaneous functions

Cornell University researchers, Ithaca, N.Y., in collaboration with a team at the Polish Academy of Sciences, have developed the first dual-sided – or “dualtronic” – chip that combines photonic and electronic functions simultaneously, an innovation that could shrink the size of functional devices, make them more energy efficient and reduce manufacturing costs.

Continue reading

Solar Manufacturing ships Mentor Pro furnaces for renewable energy applications

Solar Manufacturing, Sellersville, Pa., announced that it has shipped two Mentor Pro vacuum furnaces to a customer focused on developing advanced renewable energy technologies for large-scale industrial applications. The furnaces were selected after a collaborative process with the customer’s engineers, supported by the Research and Development team from Solar Manufacturing’s affiliate, Solar Atmospheres. The customer valued the furnace’s capabilities and compact design.

The Mentor Pro furnaces feature a molybdenum shielded hot zone, a maximum temperature capacity of 2500°F, and a workload capacity of up to 1000 pounds. They are equipped with SolarVac Essentials, a PLC-based control system, and include an internal gas quenching system with a 50 HP motor and variable frequency drive (VFD), offering flexibility in using nitrogen or argon gas for optimal metallurgical results. These features make the Mentor Pro well-suited for a variety of metallurgical applications in renewable energy development.

Read further here.

One Minute Mentor: Distortion of Ledeburitic Cold-Work Tool Steels

The different effects of steel composition on the dimensional change of plates made of ledeburitic cold-work tool steels and a working hardness of 61 HRC can be taken from the figure. Typical representatives of the new generation of improved toughness 8-9%Cr-steels show slightly higher growth in dimension than the classical 12%Cr-D2 steel. 

The growth in thickness (in the rolling direction) is always significantly higher than in width, confirming again the generally known behavior. Salt-bath heat treatment results in higher distortion than various vacuum heat treatments with high-pressure gas quenching, but the results indicate that there is also a significant scatter for gas quenching depending on the detailed quenching conditions. 

For more information, click on the link below (subscription required). Then scroll to Figure 12. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

Wisconsin Oven ships composite curing oven to Defense Industry

Wisconsin Oven, East Troy, WI, has announced the shipment of a gas-fired walk-in batch oven to a prominent manufacturer in the defense industry. The oven is designed for curing filament wound composite materials and is capable of processing a 78,000-pound load on a 40-foot long mandrel carried by a load car.

The work chamber measures 10 feet wide, 42 feet long, and 9 feet high, with a qualified work zone of 8 feet by 40 feet by 8 feet. The oven includes a rotation system to prevent drooping of uncured composites during the heating process, offering speed control flexibility through a variable frequency drive.

This oven operates at a maximum temperature of 500°F, with temperature uniformity of ±10°F at multiple setpoints. Equipped with a PLC-based Wisconsin Oven Premium Control System and an IoT system, it allows for real-time monitoring, predictive maintenance, and remote fault diagnosis.

Additional features include split-line construction for easier shipping, two powerful recirculation blowers, interior lighting, and safety-compliant railings and ladder access.

Read further here.

Ipsen USA launches service HUB Model for improved customer support

Ipsen USA, Cherry Valley, Illinois, announced the launch of its new Service HUB model, aimed at enhancing customer support across the United States. The HUB system, developed over the past two years under the leadership of Ipsen Global CEO Geoffrey Somary and currently overseen by Chief Service Officer John Dykstra, is now fully operational across the Midwest and Southeastern regions.

The HUBs are designed to offer quicker response times, with dedicated teams that provide tailored service for customers in close geographic proximity. This model allows Ipsen to optimize service efficiency, reducing downtime for heat-treating operations and improving customer experience.

In addition to benefiting customers, the HUB model also enhances the work-life balance of Ipsen’s Field Service Engineers (FSEs) by reducing travel time. The initiative is led by Lu Chouraki, Manager of Business Development, who emphasized the goal of minimizing response times and improving support for customers facing operational outages.

This strategic shift reflects Ipsen’s commitment to service excellence, offering personalized, regional expertise that both empowers its team and delivers enhanced support to customers.

Read further here. 

Nitrex celebrates 40 Years of innovation in heat treatment solutions

Nitrex, Quebec, announced that it is celebrating its 40th anniversary this year, marking four decades of growth and innovation in the heat treatment industry. Founded in 1984, Nitrex has evolved from a pioneer in controlled nitriding to a global leader offering end-to-end heat treatment solutions. The company’s technological advancements have expanded its capabilities to encompass metallurgy, engineering, process optimization, and automation.

Since 2019, under the current leadership, Nitrex has broadened its portfolio to include advanced vacuum furnaces and introduced technology for improved brake rotor performance. The company has also launched digital platforms such as QMULUS, aimed at optimizing customer processes and boosting operational efficiency.

In addition to its own milestone, Nitrex is celebrating the 50th anniversary of its UPC-Marathon office in Germany, recognizing the long-standing contributions and achievements of its global team. These anniversaries reflect Nitrex’s ongoing commitment to innovation and excellence.

Read further here.

Research to use machine learning to ‘reverse-engineer’ new composite materials

Materials science engineers often struggle to design materials that are strong in all directions, as strengthening them for one type of load can create weaknesses for another. To address this, Binghamton University Assistant Professors Mir Jalil Razavi and Dehao Liu are using artificial intelligence and machine learning to develop composite materials with specific mechanical properties. Their project, supported by a $313,087 grant from the National Science Foundation, aims to create a deep-learning model that customizes the microarchitecture of these materials based on physical laws.

“When we look at materials now, we usually tune mechanical properties in one direction,” Razavi said. “For example, they can absorb the shock in ‘x’ direction, but they don’t pay attention to what will happen to the ‘y’ or ‘z’ direction. While we strengthen in one direction, maybe we’ll compromise their mechanical properties in the other directions.”

“Imagine trying to mix two types of materials,” Liu said. “One is very solid and stiff. One is very soft, like if you mix stone and gel and then glue them together. How can you design the distribution of the stone and the gel? They can show different mechanical properties at different directions.”

Razavi and Liu will develop thousands of mechanical computational models to train deep learning algorithms in designing composite materials tailored to specific needs. They will decide which suggestions are most promising, and their collaborator, Associate Professor Yanyu Chen from the University of Louisville (Kentucky), will validate the best combinations through additive manufacturing (3D printing), X-ray imaging and stress testing.

“With this research, the goal would be that you give the material properties you are seeking in that different direction, and I inversely fabricate the material for you,” Razavi said.

The idea for the project originated from Razavi’s research on the human brain. He hopes to chart the formation of brain folds as faster-growing grey matter (the outer layer where higher-level thinking is done) grows on top of white matter (the inner layer that communicates between different gray matter areas and between the gray matter and the rest of the body).

“Because brain tissue has different fiber tracts, it shows different mechanical properties in different directions,” he said. “When we want to fully characterize brain tissue, we need multiple loading cases to analyze that.”

The Binghamton team believes this machine learning research could revolutionize materials design and enable the rapid development of new materials with tailored properties for a wide range of applications, such as designing lighter structures, effective shock absorbers and aerospace components.

“It could be used not just in advanced areas like the brain, but also everyday materials like helmets and shoes,” Liu said. “If your shoes don’t feel comfortable, you can design your own personal pair using materials with different mechanical properties.”

For more information: Binghamton University

Dr. Navin Manjooran Appointed as President of ASM International

MATERIALS PARK, Ohio (October 1, 2024) – ASM International, the world’s largest association of materials-centric engineers and scientists, proudly announces that Dr. Navin Manjooran has been appointed President of the ASM International for the 2024-2025 term. With more than two decades of global leadership and technical expertise, Dr. Manjooran brings a wealth of knowledge in materials science, engineering, and advanced technologies to this prestigious role.

Dr. Manjooran is a long-standing member of ASM, a Board of Trustees member, an ASM Fellow, and ascends to this role after recently serving as the Senior Vice President of the ASM International. In addition to his role as ASM President, Dr. Manjooran currently serves as Chairman of Solve, a global technology and research services company addressing critical energy, industry, medical, and infrastructure challenges.

His distinguished career includes nearly a decade in senior global leadership at Siemens AG, where he oversaw international collaborations, strategic development, and innovation across the Siemens portfolio. Throughout his career, he has made significant contributions to the advancement of materials science and engineering, organizing over thirty-seven international symposia, and having more than two-hundred publications or presentations. He has twelve patents or disclosures and twelve books in the field. He is a Fellow of ASM International, American Ceramic Society (ACerS), Institute of Materials, Minerals and Mining (IOM3) and Indian Institute of Metals (IIM).

Dr. Manjooran’s academic and professional accomplishments are extensive. He holds a bachelor’s degree in metallurgical engineering from the National Institute of Technology (NIT Warangal, India), a master’s degree in materials science and engineering from the University of Florida, and a doctorate in materials science and engineering from Virginia Tech. He also has an MBA from the Booth School of Business at the University of Chicago and his executive management education from Harvard University. His many accolades include the Distinguished Virginia Tech Alumnus Award (ISA) and the University of Florida Alumnus Award (MSE), among numerous others.

Beyond his contributions to ASM International, Dr. Manjooran holds leadership roles with the University of Florida, Virginia Tech, and several prestigious engineering and technology organizations worldwide. He is also an adjunct Professor of Materials Science and Engineering at Virginia Tech. He has also served on the several boards including the Virginia Tech Board of Visitors, University of Chicago Board of Trustees and on the Massachusetts Institute of Technology (MIT) energy initiative board.

Dr. Manjooran began his tenure as President of the ASM International Board of Trustees on October 1, 2024, succeeding Pradeep Goyal. ASM International members and materials science professionals globally look forward to the society’s continued growth and innovation under his leadership.

 

About ASM International

ASM International is the world’s largest and foremost professional technical society serving the information needs of scientists, engineers, and technicians who develop, test, select, and apply advanced materials, including metals, composites, polymers, and ceramics. Founded over 110 years ago, as the world’s largest and most established materials information society with 17,000+ members, ASM engages and connects members to a global network of peers and provides access to trusted materials information through reference content and data, education courses, international events, and applied research.

To learn more about ASM International, visit asminternational.org or call 440.338.5151 to speak with an ASM International representative. Follow us on Facebook, LinkedIn, and Twitter.

Metal with nanoscale voids is mechanically superior to void-free samples

A research team led by Prof. JIN Haijun from the Institute of Metal Research (IMR) of the Chinese Academy of Sciences, recently proposed a radical new way to view voids that counters the traditional perspective that fatal flaws must be eliminated in manufacturing. They suggest that the presence of voids is not always hazardous. Instead, voids can be beneficial if they are added “properly” in the material.

Continue reading