Hybrid Advanced Manufacturing of Structural Materials

For a metal additive manufactured part to achieve final geometric dimensions with required precision, the desired surface finish, and obtain specified material properties, an entire value chain of processes must be used that includes conventional materials manufacturing processes.

Continue reading

Surgical pins change color with strain

Engineers at Tufts University, Medford, Mass., created a new format of solids made from silk protein that can be preprogrammed with biological, chemical, or optical functions, such as mechanical components that change color with strain, deliver drugs, or respond to light.

Continue reading