MANA scientists usher in advances in thermoelectric materials

Thermoelectric (TE) materials convert heat into electricity and can contribute to compensating for the global fossil fuel shortage. Their conversion mechanism relies on factors such as electron and vibrational wave (phonon) scattering at grain boundaries (GB) that form between different crystal orientations in a material. Notably, some kinds of doping can show potential to optimize thermoelectric performance and enhance the heat-to-electricity conversion efficiency.

Among promising TE materials are alloys containing magnesium and antimony or bismuth, denoted as Mg3(Sb, Bi)2. Since reducing GB scattering can enhance their performance, it is worth probing how certain kinds of doping can affect these alloys.

Now, in a recent study led by Dr. Takao Mori, Group Leader of the Thermal Energy Materials Group at MANA, at the National Institute for Materials Science (NIMS), along with first author Mr. Longquan Wang, Mg3(Sb, Bi)2-based alloys were enhanced by the addition of molybdenum (Mo). The team discovered that Mo aids electron movement by regulating the grain size and band structure (allowed energy levels for electrons in a solid). They also optimized the Sb to Bi ratio to restrain phonon transport by introducing structural defects, reducing phonon group velocity and increasing atomic disorder. A single-leg device achieved close to 12% conversion efficiency.

The practical implications of this study could have substantial real-world effects. Moreover, Mg3(Sb, Bi)2-based materials use abundant and low-cost elements, unlike alloys such as PbTe and GeTe, which contain rare and toxic elements. According to Dr. Mori, “With the intensifying energy consumption and environmental issues, recovering waste heat from industry, transportation, and daily life is an important issue. Thermoelectric devices can directly convert heat into electricity, thereby providing a potential solution for the energy crisis and environmental issues.”

In summary, MANA scientists have achieved improved thermoelectric performance in Mg3(Sb, Bi)2-based materials, opening possibilities for developing materials capable of harvesting heat effectively.

For more information: Advanced Energy Materials

How fractures propagate and stop

Harvard scientists, in collaboration with an international and interdisciplinary team of researchers, are exploring how cracks start, propagate, and end. Their findings, detailed in papers published in Nature Physics and AGU Advances, provide a deeper understanding of the lifecycle of fractures and could improve our understanding of material science, earthquakes, and production of geothermal energy, oil, and gas.

Continue reading

Corrosion examined on atomic level

When water vapor meets metal, the resulting corrosion can lead to mechanical problems that harm a machine’s performance. Through passivation, it also can form a thin inert layer that acts as a barrier against further deterioration. Either way, the exact chemical reaction is not well understood on an atomic level, but that is changing thanks to environmental transmission electron microscopy (TEM), which allows researchers to directly view molecules interacting on the tiniest possible scale.

Continue reading

Scientists announce breakthrough in hypersonic heat shield

In a giant leap for future hypersonic flight, Chinese scientists have turned to multi-scale technology to develop a revolutionary new material that has achieved record high marks in tests for vital strength and thermal insulation properties.

The scientists say their porous ceramic creation opens the door to wider exploration in the fields of aerospace, chemical engineering and energy transfer and production.

“For the first time, it is reported a multi-scale structure design and fast fabrication of … high-entropy ceramics via an ultrafast high-temperature synthesis technique that can lead to exceptional mechanical load-bearing capability and high thermal insulation performance,” the researchers said.

Scientists have long faced challenges in developing strong, lightweight materials boasting low-thermal conductivity that are critical, especially for hypersonic travel. Ceramic materials offer promise because they exhibit low thermal conductivity, high melting points and corrosion resistance, and they are also non-combustible.

But exploration projects at great depths below the Earth’s surface as well as in outer space encounter extremely high temperatures and pressure. Traditional ceramic materials are insufficient in those instances.

Lightweight, porous materials offered low thermal transfer but that desirable property often came with a tradeoff—greater fragility.

In their report, “Ultrastrong and High Thermal Insulating Porous High-Entropy Ceramics up to 2000 °C,” researchers at Guangzhou University School of Materials Science and Engineering stated, “It is imperative to find ways to simultaneously improve the mechanical strength and thermal insulation capacity of porous ceramics.”

So they turned to the concept of high-entropy design to come up with a porous ceramic material that achieved a good balance between strength and heat resistance without the usual downsides.

High-entropy design focuses on the use of equal measures of multiple elements that can be used to create stronger, more heat-resistant and more stable components.

The researchers developed a material that achieved the demanding insulation and weight criteria for aerospace flight. Their new ceramic creation, which goes by the unassuming name 9PHEB—9-cation porous high-entropy diboride—provides “exceptional thermal stability” and “ultrahigh compressive strength,” the researchers said.

“High-quality interfaces, characterized by strong bonding without defects or amorphous phases, can promote the rapid force transfer along the building block and to many other ones through connections upon loading, leading to a significant enhancement of mechanical strength,” the report said.

For more information: Advanced Materials

Image: Morphology and statistics of the fabricated 9PHEB samples after acid corrosion. (a) SEM image of the samples with a porosity of ~50%. (b) Statistics of the grain sizes. The average grain size is calculated to be 1.07±0.31 μm.

Removing impurities from boron nitride nanotubes

Strong, lightweight materials that can tolerate very high temperatures have the potential to improve existing technologies, pave the way for the creation of novel biomedical imaging or hydrogen storage applications, or even usher in the next generation of spacecraft.

To do this, researchers at Rice University working with Angel Martí’s lab have discovered a novel method for creating high-purity boron nitride nanotubes, which are hollow, cylindrical structures that are stronger by weight than steel and can tolerate temperatures as high as 900 degrees Celsius (~1652 Fahrenheit).

In a study, Rice researchers found that by utilizing phosphoric acid and fine-tuning the process, they could eliminate stubborn contaminants from boron nitride nanotubes.

Boron nitride cages, which are hollow sphere-shaped structures that enclose boron particles, are the “extra stuff” that often degrades the quality and use of the nanotubes. The researchers looked into the possibility of using phosphoric acid to dissolve the cages after discovering in a study that the acid functioned as a boron nitride wetting agent.

Nothing occurred at normal temperature. However, the researchers were taken aback when they heated things up.

Martí further added, “When we looked through the microscope, we saw no tubes and no cages. Instead, there were pyramids.”

After discovering that the high temperatures and acid concentrations were harmful to the boron nitride, the researchers changed their original plan of action to modify the reaction so that it would only destroy the material’s undesirable structures.

Shumard noted, “Through a lot of experimentation, we developed a completely new direction for purification of nanotubes. I have spent a lot of time in front of an electron microscope and have read a lot of papers with images of boron nitride nanotubes. The material that we can make is by far the purest tubes that I have seen when compared to others.”

The researchers intend to keep working to increase reaction yields to generate enough nanotubes to create fibers, which could serve as a good and more environmentally friendly substitute for steel.

“Nitrogen makes up 70% of our atmosphere, and boron is highly abundant in rocks. This work could be a stepping stone to much better building materials both in terms of strength and in terms of sustainability,” Shumard added.

Both the tensile strength and thermal conductivity of boron nitride nanotubes, as well as their structure, are remarkably similar to those of carbon nanotubes. Nevertheless, compared to their carbon counterparts, boron nitride nanotubes exhibit enhanced resilience and some complementary features.

Martí stated, “For example, carbon nanotubes can be electrical conductors or semiconductors, while boron nitride nanotubes are insulators. The science on boron nitride nanotubes is not as well developed as the science on carbon nanotubes ⎯ a gap we were hoping to address in our research because we think the ability to produce pure boron nitride nanotubes efficiently and reliably could be important for a wide range of industries.”

For more information: Chemistry of Materials

Image: Scanning electron microscopy images of the starting material (from left), the material resulting from the high-concentration phosphoric acid treatment and the purified boron nitride nanotubes.Image courtesy of the Martí group/Rice University

Office of Naval Research-sponsored research could potentially lead to millions of new materials

A research team, led by the Office of Naval Research (ONR) Principal Investigator, Dr. Stefano Curtarolo, Duke University, developed a computational method for creating new types of ceramics using transition metals – carbonitrides or borides – through a process called Disordered Enthalpy-Entropy Descriptor (DEED).

The applications are endless, said Dr. Eric Wuchina, a research materials engineer who was the program officer with ONR’s Sea Warfare and Weapons department when Curtarolo’s research team was awarded the Multidisciplinary University Research Initiative (MURI).

Wuchina said. “Now we can help design any material for high voltage, breakdown resistance for strength, for high-temperature capability, for high or low thermal conductivities – a variety of things that you can do because of the thermodynamic database that Professor Curtarolo has been putting together for the last 20-25 years.”

Curtarolo’s team maintains the Duke Automatic-FLOW for Materials Database (AFLOW)—a database that allows algorithms to accurately predict the properties of unexplored mixtures without having to create them in the laboratory.

“We’ve used the same iron, copper, nickel and other alloys throughout history and just added stuff in to change the properties,” Wuchina said. “Rather than limit ourselves to just 10 chemical elements, this allows us to look at the whole periodic table of 100 elements – and to look at a variety of different compositions.”

According to Wuchina, the variety of new compositions could create potentially millions of new materials.

“Professor Curtarolo has developed the ability for us to look at a wide variety of materials and potential materials that have never been made and predict what their properties are going to be. And then how to make real materials out of those for applications for specific applications.”

So far, DEED has predicted 900 possible new formulations of high-performance materials – 17 of which have already been successfully created in laboratories.

Instead of focusing solely on the orderly atomic structure of conventional materials, Curtarolo’s team worked to develop the predictive properties of “high-entropy” materials – that is, materials that could be created through a chaotic mixture of atoms.

“The high-entropy carbides all had a relatively uniform amount of enthalpy, so we could ignore part of the equation,” Curtarolo said. “But to predict new ceramic recipes with other transition metals, we had to address the enthalpy.”

Enthalpy is a measure of the sturdiness of a design while entropy is the number of possible designs that have similar strength. Curtarolo’s computational method not only calculates what elements need to go into creating a ceramic for a certain application, but also how to arrange the microstructure – the atoms – so that it has also high-temperature capabilities.

“Typically to get higher or lower thermal conductivity you will use a ceramic,” Wuchina said. “You might make it a little more porous so that it has better-insulating properties, right? Well, how do you do that without harming the mechanical properties?”

That’s what makes Curtarolo’s research and computational method so unique. It allows him to predict how different compounds will behave and to what applications these new compounds would be best suited.

Wuchina said. “The DEED process can capture and develop a wide range of materials and the materials properties that we don’t have now, and it allows us to use computational tools to tell us what compositions and what microstructures are best and how to make them. And that’s something that has historically been trial and error.”

For more information: Nature

Tensile cracks shatter classical speed limits

Researchers at the Racah Institute of Physics, Hebrew University of Jerusalem, recently made a discovery that challenges the conventional understanding of fracture mechanics. The team, led by Dr. Meng Wang, Dr. Songlin Shi, and Prof. Jay Fineberg, experimentally demonstrated the existence of “supershear” tensile cracks that exceed classical speed limits and transition to near-supersonic velocities.

Continue reading

Ancient graphite reveals a quantum surprise

Scientists at The University of Manchester’s National Graphene Institute have discovered new physics in graphite through the application of twistronics, revealing a 2.5-dimensional mixing of surface and bulk states. The research opens new possibilities in controlling electronic properties in both 2D and 3D materials.

Continue reading

Stunning discovery: metals can heal themselves

For the first time, scientists at Sandia National Laboratories, Albuquerque, N.M. and Texas A&M University, have witnessed pieces of metal crack, then fuse back together without any human intervention, overturning fundamental scientific theories in the process.

Continue reading

Imec first to demonstrate conductor films on 300 mm wafers with lower resistivity than Cu and Ru

Imec, Belgium, a world-leading research and innovation hub in nanoelectronics and digital technologies, provided the first experimental evidence that the resistivity of a thin conductor film on a 300mm Si wafer can be lower than that of Cu and Ru, which are currently used in interconnect metallization schemes, marking a milestone towards enabling low-resistive interconnect with line widths below 10nm.

Continue reading

New invention for more efficient atomic force microscopes

Researchers at Vienna University of Technology, Austria, developed an atomic force microscope sensor element of with a customized electronic circuit built directly into the tip whose signal directly provides information about the state of the tip, producing a more compact, simpler to process, cheaper technology with precision just as good as with previous devices.

Continue reading

RoodMicrotec and SGA enter into cooperation for ASIC testing

RoodMicrotec, Netherlands, a leading independent company for semiconductors supply and quality services, and Svenska Grindmatriser AB, Sweden, a well-established fabless IDM for the development and supply of customized mixed-signal ASICs, started a cooperation for high-volume production testing of SGA’s ASIC products.

Continue reading