Using a custom-built machine to launch microprojectiles at supersonic speeds, Cornell researchers, Ithaca, N.Y., have uncovered new details about how high-speed metallic collisions can form strong, durable atomic bonds, offering insights that could enhance 3D printing and other manufacturing techniques.
Continue readingORNL research aims to support production of large-scale components
Researchers at the US Department of Energy’s Oak Ridge National Laboratory (ORNL) in Tennessee are leveraging advanced manufacturing techniques, such as Hot Isostatic Pressing (HIP) Powder Metallurgy and Additive Manufacturing, to produce parts weighing over 4,500 kg. ORNL highlights the urgent need for these large-scale components across various sectors, including aerospace, defense, nuclear, oil, gas, renewables, and construction. This demand is particularly pressing in the US, where traditional manufacturing methods like casting and forging have declined and moved overseas, leading to supply-chain shortages.
Senior research scientists Jason Mayeur and Soumya Nag are hoping to add Wire Arc Additive Manufacturing (WAAM), hybrid manufacturing, in-situ monitoring and advanced computational modeling to HIP technology to create molds faster and more accurately whilst leveraging the PM technology American manufacturers may be more acquainted with.
“PM-HIP is a vital pathway for diversifying the supply chain for producing large-scale metal parts that are becoming more difficult to source via conventional means,” Mayeur explained. “The technology is of particular interest to the nuclear and hydroelectric industrial sectors, as well as the Department of Defense.”
In contrast with traditional casting and forging techniques, PM-HIP involves fabricating pre-formed, hollow molds for each large-scale component and filling them with metal powder. Once the additively manufactured mold (aka a ‘can’ or ‘capsule’) receives an initial seal, any gas remaining inside is pumped out. Then, a more permanent hermetic seal is applied.
At this point, the capsule is heated and pressurized in prescribed cycles within a Hot Isostatic Press (essentially a pressurized furnace). Without melting, these cycles facilitate the consolidation of the metal powder into the required shape in a process exchange of heat and pressure known as solid-state bonding. When bonding is complete, acid leaching or machining is used to remove the exterior can, revealing the intended part.
Jason Mayeur works in the Deposition Science and Technology Group at ORNL, where he applies his knowledge in computational solid mechanics to manufacturing challenges. His two-decade research career began with the use of computational models to understand the relationships between materials microstructure and performance. He has since segued into the analysis of the structural material performance of metals and alloys.
In this arena, Mayeur develops theory, writes code to implement his theories, and then performs simulations of solids under various loading conditions to determine their suitability for use in a variety of applications. In short, Mayeur’s code can be used to improve the PM-HIP process, thus making it a more attractive alternative to traditional casting and forging.
Soumya Nag, Mayeur’s colleague at ORNL, works in the Materials Science and Technology Division, applying his own two decades of research experience in materials and manufacturing. Nag is a metallurgist with expertise in evaluating lightweight, high-temperature structural alloys fabricated via conventional and advanced manufacturing techniques.
“Jason is an expert in predictive modeling of deformation characteristics of Hot Isostatic Pressing canisters. I am more involved in the experimental side of things. Jason and I complement each other, and really, our two efforts are very much intertwined and critical toward the overall success of the task,” Nag said.
Nag’s research centers on the processing and materials science of HIP capsule fabrication, using various additive manufacturing techniques and assessing the quality of the resulting component parts.
“Additive Manufacturing offers unique design flexibility, which, combined with the reliability of PM-HIP, can pave the path toward precise manufacturing of large-scale, custom and complex, energy-related parts while also taking advantage of multi-material builds,” he explained.
Nag collaborates with Mayeur to design and perform experiments that characterize the metal powder material’s behavior and its mechanical properties in pursuit of a better, more accurate build while providing the necessary material property inputs for Mayeur’s computational models.
Mayeur’s work targets many technological challenges posed by the PM-HIP process, striving for quality and consistency in geometry to achieve dimensional accuracy at a very large scale. One challenge is shrinkage. During PM-HIP, the volume of metal powder within the can shrinks by approximately 30%, but not uniformly.
To address these inconsistencies, Mayeur’s computational models work to predict how the shrinkage occurs for different part geometries and capsule designs. This is an iterative process that occurs after initial capsule design, using the simulation results as a guide to modify the final design.
For more information: Oak Ridge National Laboratory (ORNL)
Image: This additively manufactured PM-HIP will be used to create an impeller for a hydropower impeller, demonstrating a new approach for creating large-scale clean energy components. (Courtesy Carlos Jones/ORNL, US DoE)
Developing New High-Performance and Recyclable Materials
Professor Chiyoung Park of the Department of Energy Science and Engineering at DGIST has developed a groundbreaking new material poised to advance high-sensitivity recyclable sensor technology. Working in collaboration with Professor U-hyeok Choi of Inha University, Park’s team created a recyclable high-sensitivity sensor based on the dynamic polymer network. This next-generation material is garnering attention for its ability to combine environmental sustainability with high performance.
Existing high-sensitivity sensors have been limited by performance degradation due to fatigue and repeated use.
However, the dynamic polymer network developed by the research team maintains excellent sensitivity and durability by using vinylogous urethane bonding.
This bonding structure self-heals in response to external stimuli such as temperature, light, and pressure, preventing performance degradation even after repeated use.
The dynamic polymer network is also sensitive to various mechanical movements, heat, and light, and sensors based on the network excel at detecting human body movements.
Researchers have demonstrated that the sensors can accurately detect finger bends, changes in facial expressions, and even swallowing movements in the throat.
One of the biggest strengths of the technology is that it can maintain the same sensitivity after recycling without any degradation.
Addressing the growing issue of e-waste, the team designed the technology to combine recyclability with high performance.
They believe the dynamic polymer network’s versatility supports repeated use and recycling, potentially leading to significant reductions in e-waste.
Their work promises to have far-reaching implications not only in sensor technology but also in next-generation electronics, wearable devices, and medical equipment.
The team continues to work on commercializing the technology for widespread industrial applications.
“Our material offers excellent processability and can be recycled mechanically or chemically,” said DGIST Professor Chiyoung Park.
“The polymer network undergoes a simple recycling process, which we expect will extend the lifespan of electronic devices and wearable sensors, significantly reducing electronic waste.”
For more information: Chemical Engineering Journal
Engineering perovskite materials at the atomic level paves way for new lasers, LEDs
Researchers have developed a technique to engineer layered hybrid perovskites (LHPs) down to the atomic level, precisely controlling how these materials convert electrical charge into light. This advancement paves the way for creating materials tailored for next-generation printed LEDs and lasers, and holds promise for engineering other materials for photovoltaic devices.
Perovskites, known for their crystalline structure, possess desirable optical, electronic, and quantum properties. LHPs are composed of thin sheets of perovskite semiconductor material separated by organic spacer layers, which can be laid down as thin films. These materials are highly efficient at converting electrical charge into light, making them ideal for use in next-generation LEDs, lasers, and photonic integrated circuits. Despite their potential, understanding how to engineer LHPs to control their performance characteristics has been a challenge for researchers until now.
To understand what the researchers discovered, you have to start with quantum wells, which are sheets of semiconductor material sandwiched between spacer layers.
“We knew quantum wells were forming in LHPs – they’re the layers,” says Aram Amassian, corresponding author of a paper on the work and a professor of materials science and engineering at North Carolina State University.
And understanding the size distribution of quantum wells is important because energy flows from high-energy structures to low-energy structures at the molecular level.
“A quantum well that is two atoms thick has higher energy than a quantum well that is five atoms thick,” says Kenan Gundogdu, co-author of the paper and a professor of physics at NC State. “And in order to get energy to flow efficiently, you want to have quantum wells that are three and four atoms thick between the quantum wells that are two and five atoms thick. You basically want to have a gradual slope that the energy can cascade down.”
“But people studying LHPs kept running into an anomaly: the size distribution of quantum wells in an LHP sample that could be detected via X-ray diffraction would be different than the size distribution of quantum wells that could be detected using optical spectroscopy,” Amassian says.
“For example, diffraction might tell you that your quantum wells are two atoms thick, as well as there being a three-dimensional bulk crystal,” Amassian says. “But spectroscopy might tell you that you have quantum wells that are two atoms, three atoms, and four atoms thick, as well as the 3D bulk phase.
“So, the first question we had was: why are we seeing this fundamental disconnect between X-ray diffraction and optical spectroscopy? And our second question was: how can we control the size and distribution of quantum wells in LHPs?”
Through a series of experiments the researchers discovered that there was a key player involved in answering both questions: nanoplatelets.
“Nanoplatelets are individual sheets of the perovskite material that form on the surface of the solution we use to create LHPs,” Amassian says. “We found that these nanoplatelets essentially serve as templates for layered materials that form under them. So, if the nanoplatelet is two atoms thick, the LHP beneath it forms as a series of two-atom-thick quantum wells.
“However, the nanoplatelets themselves aren’t stable, like the rest of the LHP material. Instead, the thickness of nanoplatelets keeps growing, adding new layers of atoms over time. So, when the nanoplatelet is three atoms thick, it forms three-atom quantum wells, and so on. And, eventually, the nanoplatelet grows so thick that it becomes a three-dimensional crystal.”
This finding also resolved the longstanding anomaly about why X-ray diffraction and optical spectroscopy were providing different results. Diffraction detects the stacking of sheets and therefore does not detect nanoplatelets, whereas optical spectroscopy detects isolated sheets.
“What’s exciting is that we found we can essentially stop the growth of nanoplatelets in a controlled way, essentially tuning the size and distribution of quantum wells in LHP films,” Amassian says. “And by controlling the size and arrangement of the quantum wells, we can achieve excellent energy cascades – which means the material is highly efficient and fast at funneling charges and energy for the purposes of laser and LED applications.”
When the researchers found that nanoplatelets played such a critical role in the formation of perovskite layers in LHPs, they decided to see if nanoplatelets could be used to engineer the structure and properties of other perovskite materials – such as the perovskites used to convert light into electricity in solar cells and other photovoltaic technologies.
“We found that the nanoplatelets play a similar role in other perovskite materials and can be used to engineer those materials to enhance the desired structure, improving their photovoltaic performance and stability,” says Milad Abolhasani, co-author of the paper and ALCOA Professor of Chemical and Biomolecular Engineering at NC State.
For more information: Matter
New technology improves structural strength
Researchers from Texas A&M University and Sandia National Laboratories have significantly enhanced interlocking metasurfaces (ILMs) using shape memory alloys (SMAs), offering a stronger and more stable alternative to traditional joining techniques like bolts and adhesives, with potential applications in aerospace, robotics, and biomedical devices.
“ILMs are poised to redefine joining technologies across a range of applications, much like Velcro did decades ago,” said Dr. Ibrahim Karaman, professor and head of the Department of Materials Science and Engineering Department at Texas A&M. “In collaboration with Sandia National Laboratories, the original developers of ILMs, we have engineered and fabricated ILMs from shape memory alloys. Our research demonstrates that these ILMs can be selectively disengaged and re-engaged on demand while maintaining consistent joint strength and structural integrity.”
Similar to Legos or Velcro, ILMs enable the joining of two bodies by transmitting force and constraining movement. Until now, this joining method has been passive, requiring force for engagement.
Control of joining technology through temperature changes opens new possibilities for smart, adaptive structures without loss in strength or stability and with increased options for flexibility and functionality.
“Active ILMs have the potential to revolutionize mechanical joint design in industries requiring precise, repeatable assembly and disassembly,” said Abdelrahman Elsayed, graduate research assistant in the materials science and engineering department at Texas A&M.
Practical applications include designing reconfigurable aerospace engineering components where parts must be assembled and disassembled multiple times. Active ILMs could also provide flexible and adaptable joints for robotics-enhancing functionality. In biomedical devices, the ability to adjust implants and prosthetics to body movements and temperatures could offer a better option for patients.
The current findings utilized the shape memory effect of SMAs to recover the ILMs’ shape by adding heat. The researchers hope to build on these findings by using the superelasticity effect of SMAs to create ILMs that can withstand large deformation and instantaneously recover under very high-stress levels.
“We anticipate that incorporating SMAs into ILMs will unlock numerous future applications, though several challenges remain,” said Karaman. “Achieving superelasticity in complex 3D-printed ILMs will enable localized control of structural stiffness and facilitate reattachment with high locking forces. Additionally, we expect this technology to address longstanding challenges associated with joining techniques in extreme environments. We are highly enthusiastic about the transformative potential of ILM technology.”
For more information: Materials & Design
Image: Two proposed versions of ILMs in their different engagement states.
Novel technique for observing atomic-level changes could unlock potential of quantum materials
A research team from the Department of Energy’s Oak Ridge National Laboratory has developed the Rapid Object Detection and Action System (RODAS), a unique method that combines imaging, spectroscopy, and microscopy to observe changes in materials at the atomic level. This technique offers new opportunities for understanding and developing advanced materials for quantum computing and electronics by capturing the properties of fleeting atomic structures as they form, providing unprecedented insights into the evolution of material properties at the smallest scales.
Traditional approaches combining scanning transmission electron microscopy, or STEM, with electron energy loss spectroscopy, or EELS, have been limited because the electron beam can change or degrade the materials being analyzed. That dynamic often causes scientists to measure altered states rather than the intended material properties. RODAS overcomes the limitation and also integrates the system with dynamic computer-vision-enabled imaging, which uses real-time machine learning.
When analyzing the specimen, RODAS focuses only on areas of interest. This approach enables rapid analysis—in seconds or milliseconds—compared with sometimes several minutes that can be required by other STEM-EELS methods. Importantly, RODAS extracts crucial information without destroying the sample.
All materials have defects, and these defects can directly influence virtually any of a material’s properties—whether electronic, mechanical or quantum, for example. Defects can arrange themselves in a variety of ways at the atomic level, both intrinsically and in response to external stimuli, such as electron beam irradiation.
Unfortunately, the local properties of these various defect configurations are not well understood. Although STEM methods can experimentally measure such configurations, investigating specific configurations without altering them is extremely challenging.
“Understanding defect configurations is crucial for developing next-generation materials,” said the study’s lead author, Kevin Roccapriore of ORNL’s Center for Nanophase Materials Sciences. “If empowered with that knowledge, we could intentionally create a specific configuration to produce a specific property. Such work is entirely separate from the observation and analysis activity but represents one potentially impactful direction for the future.”
The research team demonstrated their technique on single-layer molybdenum disulfide, a promising semiconductor material for quantum computing and optics applications. Molybdenum disulfide is particularly interesting because it can emit single photons from defects known as single sulfur vacancies.
In this material, a single sulfur vacancy refers to the absence of one sulfur atom from its honeycombed lattice structure, which is the arrangement of the atoms. These vacancies can aggregate, creating unique electronic properties that make molybdenum disulfide valuable for advanced technological applications.
By studying molybdenum disulfide and similar single-layer materials, scientists hope to answer vital questions about optical or electronic properties at the atomic scale.
The RODAS technique represents a significant leap forward in materials characterization. It empowers researchers to dynamically explore structure-property relationships during analysis, target specific atoms or defects for measurement as they form, efficiently collect data on various defect types, adapt to identify new atomic or defect classes in real time and minimize sample damage while maintaining detailed analysis.
By applying this technology to a single layer of vanadium-doped molybdenum disulfide, the research team gained new understanding of defect formation and evolution under electron beam exposure. This approach allows for exploring and characterizing materials in dynamic states, offering a deeper knowledge of how materials behave under various stimuli.
“Materials science techniques such as advanced electron microscopy continue to expand our comprehension of the physical world, and systems such as RODAS could play a crucial role in accelerating discovery and innovation,” Roccapriore said.
“The ability to observe and analyze materials at the atomic scale in real time shows potential for pushing the boundaries in computing, electronics and beyond, and ultimately enabling the development of transformative technologies.”
For more information: Science Advances
Image: Electron microscopy measurements are usually performed by collecting all points in a 2D grid. Here, using deep learning in real time, only sites of interest are measured (colored circles), allowing experiments to be conducted on a much larger variety of materials, even those that change under the beam.
Materials Analysis Technology releases a MOU with SGS
Materials Analysis Technology Inc., Taiwan, and Swiss SGS Taiwan Ltd. signed a memorandum of understanding with the goal of providing comprehensive ISO 26262 functional safety product certification services, AEC-Q automotive electronic component reliability verification services, and soft error rate assessment and analysis in the automotive semiconductor and electronic component industries in Taiwan.
Continue readingFaraday enhances 3D-IC design service with Ansys multiphysics analysis
Faraday Technology Corporation, Pittsburgh, Pa., a leading application specific integrated circuits (ASIC) design service and IP provider, is expanding its use of Ansys technology to enhance its capabilities in developing advanced designs for multi-die 2.5D/3D-ICs — critical for artificial intelligence (AI), IoT, and 5G applications. With support from Ansys, Faraday will empower its customers to explore more robust design options for more innovative products.
Faraday recently announced a 2.5D/3D-IC advanced package service to address exploding demand for multi-die designs that target products with better performance and lower power consumption. To meet this demand, engineers need the right multiphysics analysis tools to verify that chip designs include reliable signal and structural integrity and reliable power distribution before it goes to fabrication. This challenge is compounded by the trend toward developing denser chips that are more vulnerable to EM issues.
Adding RaptorX into the design flow will enable Faraday to increase precision and efficiency in its development process. Moreover, it enables predictively accurate EM modeling and analysis for advanced 3D-IC products, ensuring data transfer meets stringent modern standards. This will improve the design’s fidelity, enhance performance and reliability, and accelerate time-to-market.
“Our extensive silicon IP allows our customers to start designing from a solid foundation, enabling them to focus solely on innovation and differentiating themselves in the market,” said C.H. Chien, vice president of R&D at Faraday. “Fabrication is exceptionally expensive and there is no room for error. So, keeping the overall project cost low is paramount, and it starts with the initial design. With the addition of RaptorX in this phase, we can offer customers an efficient workflow that includes design verification and signoff as well as access to top-tier test and fabrication services, removing doubts about the chip’s performance and longevity.”
“Ansys’ focus on multiphysics platforms enables innovators like Faraday to address key challenges for 3D-IC and accelerate their time-to-market,” said John Lee, vice president and general manager of the semiconductor, electronics, and optics business unit at Ansys. “Our industry-leading tools facilitate meticulous modeling and analysis of electromagnetic phenomena, helping our customers remain at the forefront of technological advancements in 5G, AI, and IoT.”
Image – EMag extraction of an interposer lane, including 48 signals in the presence of their respective VDD/VSS network and indicative simulation results, and S-Parameter analysis and transient (eye diagram) analysis of a signal line.
For more information:
Ansys
Faraday Technology Corporation
Water-free manufacturing approach could advance 2D electronics integration
A team of academic and enterprise researchers at Penn State has developed a synthesis process to produce a “rust-resistant” coating with additional properties ideal for creating faster, more durable electronics.
Continue readingThere’s two sides to this semiconductor, and many simultaneous functions
Cornell University researchers, Ithaca, N.Y., in collaboration with a team at the Polish Academy of Sciences, have developed the first dual-sided – or “dualtronic” – chip that combines photonic and electronic functions simultaneously, an innovation that could shrink the size of functional devices, make them more energy efficient and reduce manufacturing costs.
Continue readingOrdered defects may be key for solution-deposited semiconductors
Researchers at the University of Illinois Urbana-Champaign discovered that ordered defect pairs in solution-deposited semiconductors lead to record-high transistor performance, challenging conventional wisdom in semiconductor manufacturing.
Continue readingResearch to use machine learning to ‘reverse-engineer’ new composite materials
Materials science engineers often struggle to design materials that are strong in all directions, as strengthening them for one type of load can create weaknesses for another. To address this, Binghamton University Assistant Professors Mir Jalil Razavi and Dehao Liu are using artificial intelligence and machine learning to develop composite materials with specific mechanical properties. Their project, supported by a $313,087 grant from the National Science Foundation, aims to create a deep-learning model that customizes the microarchitecture of these materials based on physical laws.
“When we look at materials now, we usually tune mechanical properties in one direction,” Razavi said. “For example, they can absorb the shock in ‘x’ direction, but they don’t pay attention to what will happen to the ‘y’ or ‘z’ direction. While we strengthen in one direction, maybe we’ll compromise their mechanical properties in the other directions.”
“Imagine trying to mix two types of materials,” Liu said. “One is very solid and stiff. One is very soft, like if you mix stone and gel and then glue them together. How can you design the distribution of the stone and the gel? They can show different mechanical properties at different directions.”
Razavi and Liu will develop thousands of mechanical computational models to train deep learning algorithms in designing composite materials tailored to specific needs. They will decide which suggestions are most promising, and their collaborator, Associate Professor Yanyu Chen from the University of Louisville (Kentucky), will validate the best combinations through additive manufacturing (3D printing), X-ray imaging and stress testing.
“With this research, the goal would be that you give the material properties you are seeking in that different direction, and I inversely fabricate the material for you,” Razavi said.
The idea for the project originated from Razavi’s research on the human brain. He hopes to chart the formation of brain folds as faster-growing grey matter (the outer layer where higher-level thinking is done) grows on top of white matter (the inner layer that communicates between different gray matter areas and between the gray matter and the rest of the body).
“Because brain tissue has different fiber tracts, it shows different mechanical properties in different directions,” he said. “When we want to fully characterize brain tissue, we need multiple loading cases to analyze that.”
The Binghamton team believes this machine learning research could revolutionize materials design and enable the rapid development of new materials with tailored properties for a wide range of applications, such as designing lighter structures, effective shock absorbers and aerospace components.
“It could be used not just in advanced areas like the brain, but also everyday materials like helmets and shoes,” Liu said. “If your shoes don’t feel comfortable, you can design your own personal pair using materials with different mechanical properties.”
For more information: Binghamton University
Metal with nanoscale voids is mechanically superior to void-free samples
A research team led by Prof. JIN Haijun from the Institute of Metal Research (IMR) of the Chinese Academy of Sciences, recently proposed a radical new way to view voids that counters the traditional perspective that fatal flaws must be eliminated in manufacturing. They suggest that the presence of voids is not always hazardous. Instead, voids can be beneficial if they are added “properly” in the material.
Continue readingINBRAIN Neuroelectronics announces world’s first human graphene-based Brain computer Interface procedure
“The world’s first human application of a graphene-based BCI highlights the transformative impact of graphene-based neural technologies in medicine. This clinical milestone opens a new era for BCI technology, paving the way for advancements in both neural decoding and its application as a therapeutic intervention,” said Carolina Aguilar, CEO and Co-Founder of INBRAIN Neuroelectronics.
INBRAIN’s BCI platform leverages the exceptional properties of graphene, a material made of a single layer of carbon atoms. Despite being the thinnest known material to science, graphene is stronger than steel and possesses a unique combination of electronic and mechanical properties that make it ideal for neurotechnology innovation.
“We are capturing brain activity in areas where traditional metals and materials struggle with signal fidelity. Graphene provides ultra-high density for sensing and stimulating, which is critical to conduct high precision resections while preserving the patient’s functional capacities, such as movement, language or cognition,” said Dr. David Coope, the neurosurgeon who performed the procedure.
“After extensive engineering development and pre-clinical trials, INBRAIN’s first-in-human study will involve 8-10 patients, primarily to demonstrate the safety of graphene in direct contact with the human brain,” said Kostas Kostarelos, Ph.D., Co-Founder, INBRAIN Neuroelectronics. “The study will also aim to demonstrate graphene’s superiority over other materials in decoding brain functionality in both awake and asleep states.”
“The integration of graphene and AI with advanced semiconductor technology has allowed INBRAIN to pioneer a new generation of minimally-invasive BCI therapeutics designed for the personalized treatment of neurological disorders,” said Jose A. Garrido, Ph.D., Co-Founder and Chief Scientific Officer of INBRAIN and ICREA Professor at the Catalan Institute of Nanoscience and Nanotechnology.
The study is powered by INBRAIN’s graphene-based Intelligent Network Decoding & Modulation (BCI-Tx) Platform, which has received Breakthrough Device Designation for Parkinson’s disease from the U.S. Food & Drug Administration. INBRAIN’s BCI-Tx platform leverages graphene’s unique properties to deliver ultra-high signal resolution and adaptive neuroelectronic therapy, enabling real-time decoding of biomarkers and precise modulation of cortical and subcortical structures at the micrometer scale for neural network rebalancing.
For more information: INBRAIN Neuroelectronics
‘Writing’ with atoms could transform materials fabrication for Quantum devices
Scientists at the Department of Energy’s Oak Ridge National Laboratory have developed a groundbreaking advanced microscopy tool that can precisely place individual atoms, enabling the creation of new materials with unique properties for quantum computing and communication devices that cannot be produced by conventional methods.
“By working at the atomic scale, we also work at the scale where quantum properties naturally emerge and persist,” said Stephen Jesse, a materials scientist who leads this research and heads the Nanomaterials Characterizations section at ORNL’s Center for Nanophase Materials Sciences, or CNMS. “We aim to use this improved access to quantum behavior as a foundation for future devices that rely on uniquely quantum phenomena, like entanglement, for improving computers, creating more secure communications and enhancing the sensitivity of detectors.”
To accomplish improved control over atoms, the research team created a tool they call a synthescope for combining synthesis with advanced microscopy. The researchers used a scanning transmission electron microscope, or STEM, transformed into an atomic-scale material manipulation platform. The synthescope will advance the state of the art in fabrication down to the level of the individual building blocks of materials. This new approach allows researchers to place different atoms into a material at specific locations; the new atoms and their locations can be selected to give the material new properties.
“Classical computers use bits, which can be either 0 or 1, and do calculations by flipping these bits,” said ORNL’s Ondrej Dyck, a materials scientist contributing to the research. “Quantum computers use qubits, which can be both 0 and 1 at the same time. The qubits can also become entangled, with one qubit connected to the state of another. This entangled system of qubits can be used to solve certain problems much faster than classical computers. The tricky part is keeping these delicate qubits stable and working correctly in the real world.
“One strategy to tackle these challenges is to build and operate at the scale where quantum mechanics exist more naturally—at the atomic scale. We realized that if we have a microscope that can resolve atoms, we may be able to use the same microscope to move atoms or alter materials with atomic precision. We also want to be able to add atoms to the structures we create, so we need a supply of atoms. The idea morphed into an atomic-scale synthesis platform—the synthescope.”
That is important because the ability to tailor materials atom-by-atom can be applied to many future technological applications in quantum information science, and more broadly in microelectronics and catalysis, and for gaining a deeper understanding of materials synthesis processes. This work could facilitate atomic-scale manufacturing, which is notoriously challenging.
“Simply by the fact that we can now start putting atoms where we want, we can think about creating arrays of atoms that are precisely positioned close enough together that they can entangle, and therefore share their quantum properties, which is key to making quantum devices more powerful than conventional ones,” Dyck said.
Such devices might include quantum computers — a proposed next generation of computers that may vastly outpace today’s fastest supercomputers; quantum sensors; and quantum communication devices that require a source of a single photon to create a secure quantum communications system.
By using an electron beam, or e-beam, to remove and deposit the atoms, the ORNL scientists could accomplish a direct writing procedure at the atomic level.
“The process is remarkably intuitive,” said ORNL’s Andrew Lupini, STEM group leader and a member of the research team. “STEMs work by transmitting a high-energy e-beam through a material. The e-beam is focused to a point smaller than the distance between atoms and scans across the material to create an image with atomic resolution. However, STEMs are notorious for damaging the very materials they are imaging.”
The scientists realized they could exploit this destructive “bug” and instead use it as a constructive feature and create holes on purpose. Then, they can put whatever atom they want in that hole, exactly where they made the defect. By purposely damaging the material, they create a new material with different and useful properties.
“We’re exploring methods to create these defects on demand so we can place them where we want to,” Jesse said. “Since STEMs have atomic-scale imaging capabilities, and we work with very thin materials that are only a few atoms in thickness, we can see every atom. So, we are manipulating matter at the atomic scale in real time. That’s the goal, and we are actually achieving it.”
For more information: Nano Letters
Image: This artistic rendering shows a way to make materials atom-by-atom. The electron beam ejects a carbon atom from graphene, and a different atom bonds at the vacancy.
Make them thin enough, and antiferroelectric materials become ferroelectric
Get the latest on titanium brazing
An article by one of the leading authorities on titanium brazing – vetted and accepted for publication in the peer-reviewed ASM Handbook, Volume 6, Welding, Brazing, and Soldering – is now available online in digital form. “Brazing of Conventional Titanium Alloys,” a comprehensive, fact-filled survey by industry expert Alexander E. Shapiro, Ph.D., Titanium Brazing Inc., offers in-depth analysis and practical advice on how to braze commercially pure and alloyed titanium with itself as well as with other materials such as copper, stainless steel, carbon steel, ceramics, graphite, and titanium aluminide.
Continue readingNomination deadline for the 2016 Class of Fellows is fast approaching
The honor of Fellow of the Society was established to provide recognition to members for distinguished contributions in the field of materials science and engineering, and to develop a broadly based forum for technical and professional leaders to serve as advisors to the Society. The deadline for submission is November 30.
Continue readingBruker introduces next generation benchtop stylus profilometer
Bruker Corporation, Billerica, Mass., released the Dektak Pro stylus profilometer, the next-generation profiler in the industry-leading Dektak product line, expanding measurement area and accuracy for critical analyses.
Continue readingNewly discovered role of phase separation: a game changer for AI memory tech
Researchers on a team led by University of Michigan unveiled that phase separation, alongside oxygen diffusion, crucially supports the long-term retention of information in memristors, specifically in resistive random access memory.
Continue readingNew chip may lead to AI computing at light speed
Engineers at the University of Pennsylvania, Philadelphia, developed a new chip that uses light waves rather than electricity to perform the complex math essential to training AI.
Continue readingResearch sheds light on universal mechanisms of work hardening
Scientists from the Harvard John A. Paulson School of Engineering and Applied Sciences (SEAS) have, for the first time, observed the detailed mechanisms of work hardening, a process discovered by early blacksmiths in the Bronze and Iron Ages that strengthens metal through deformation. This research, conducted at the Harvard Materials Research Science and Engineering Center (MRSEC), enhances our understanding of material strength and could significantly impact material design and manufacturing, where work hardening is still widely used to strengthen various products, from car frames to power wires.
“Work hardening is used in many industrial deformation processes,” said Frans Spaepen, John C. and Helen F. Franklin Professor of Applied Physics at SEAS and senior author of the study. “Today, large-scale computer programs are used to model work hardening, but if you want to make those models as effective as possible, we need to know more about the underlying laws that govern that process. This work gives us a real-time window into the universal process of work hardening.”
It’s been impossible to observe work hardening in metals in real time because the atomic structures can only be observed through an electron microscope. Researchers can compare the structure before and after deformation but have had only a limited view of what happens during the process. Previous research has revealed that imperfections in the structure, known as dislocations, form a network of defects that cause the work hardening.
“What hasn’t been clear is the full complexity of the interactions between the defects in these atomic crystals that lead to hardening,” said Ilya Svetlizky, a former SEAS postdoctoral fellow with the MRSEC and co-first author of the paper.
To understand that critical part of the process, the research team turned to colloidal crystals—particles that are about 10,000 times larger than atoms and spontaneously form a crystal structure at high concentrations. These crystals mimic atomic systems because they have the same structures, undergo the same phase transitions, and possess the same types of defects. Colloidal crystals, however, are very soft—even 100,000 times softer than Jell-O.
The researchers grew these colloidal crystals composed of millions of particles and observed each particle using a confocal optical microscope. When they applied a strain to these crystals, they could measure the motion of each and every particle.
Surprisingly, these colloidal crystals experience significant work hardening—even more strongly than any other material. In fact, when the difference in particle size is taken into account, these ultra-soft materials become much stronger than most metals.
“We did not expect that hard-sphere colloidal crystals could work hardened,” said Seongsoo Kim, an MRSEC-supported graduate student of Spaepen and Weitz and co-first author of the paper. “The interactions between particles are too simple compared to normal metals. In fact, we found that these soft materials exhibit exceptionally pronounced work hardening, even more so than most metals like copper and aluminum.”
It is the first time that work hardening has been observed in colloidal crystals; it reveals that the process is governed primarily by the geometry of the particles and the defects. The crystals became stronger because of the dislocation defects and how they interact and entangle with one another.
These observations reveal the universal mechanisms of work hardening, which will also apply more generally to all materials, even those that cannot be studied with optical microscopes. These soft colloidal crystals exhibit such exceptionally large work hardening because they can contain a very high density of these defects.
“This research tells us something fundamental and universal about how materials get stronger. These are amazing materials: Even though they are very soft, work hardening makes them into the strongest materials known,” said David A. Weitz, Mallinckrodt Professor of Physics and of Applied Physics, and a co-author of the paper.
For more information: Nature
Image: Plastic shear deformation of colloidal single crystals.
Molecular simulations, supercomputing lead to energy-saving biomaterials breakthrough
A team of scientists at the Department of Energy’s Oak Ridge National Laboratory has developed a new method to process nanocellulose, a plant-based material, reducing energy needs by 21%. This method, discovered through molecular simulations and pilot testing, uses a solvent of sodium hydroxide and urea in water, significantly lowering production costs of nanocellulosic fiber, a strong, lightweight biomaterial ideal for 3D-printing sustainable structures. The findings, achieved in collaboration with the University of Tennessee and the University of Maine, support a circular bioeconomy by replacing petroleum-based resources with renewable, biodegradable materials, thus decarbonizing the economy and reducing waste.
The scientists pursued more efficient fibrillation, the process of separating cellulose into nanofibrils, traditionally an energy-intensive, high-pressure mechanical procedure occurring in an aqueous pulp suspension. The researchers tested eight candidate solvents to determine which would function as a better pretreatment for cellulose. They used computer models that mimic the behavior of atoms and molecules in the solvents and cellulose as they move and interact. The approach simulated about 0.6 million atoms, giving scientists an understanding of the complex process without the need for initial, time-consuming physical work in the lab.
The simulations developed by researchers with the UT-ORNL Center for Molecular Biophysics, or CMB, and the Chemical Sciences Division at ORNL were run on the Frontier exascale computing system — the world’s fastest supercomputer for open science. Frontier is part of the Oak Ridge Leadership Computing Facility, a DOE Office of Science user facility at ORNL.
“These simulations, looking at every single atom and the forces between them, provide detailed insight into not just whether a process works, but exactly why it works,” said project lead Jeremy Smith, director of the CMB and a UT-ORNL Governor’s Chair.
Once the best candidate was identified, the scientists followed up with pilot-scale experiments that confirmed the solvent pretreatment resulted in an energy savings of 21% compared to using water alone.
With the winning solvent, researchers estimated an electricity savings potential of about 777-kilowatt hours per metric ton of cellulose nanofibrils, or CNF, which is roughly the equivalent of the amount needed to power a house for a month. Testing of the resulting fibers at the Center for Nanophase Materials Science, a DOE Office of Science user facility at ORNL, and U-Maine found similar mechanical strength and other desirable characteristics compared with conventionally produced CNF.
“We targeted the separation and drying process since it is the most energy-intense stage in creating nanocellulosic fiber,” said Monojoy Goswami of ORNL’s Carbon and Composites group. “Using these molecular dynamics simulations and our high-performance computing at Frontier, we were able to accomplish quickly what might have taken us years in trial-and-error experiments.”
“When we combine our computational, materials science and manufacturing expertise and nanoscience tools at ORNL with the knowledge of forestry products at the University of Maine, we can take some of the guessing game out of science and develop more targeted solutions for experimentation,” said Soydan Ozcan, lead for the Sustainable Manufacturing Technologies group at ORNL.
The project is supported by both the DOE Office of Energy Efficiency and Renewable Energy’s Advanced Materials and Manufacturing Technologies Office, or AMMTO, and by the partnership of ORNL and U-Maine known as the Hub & Spoke Sustainable Materials & Manufacturing Alliance for Renewable Technologies Program, or SM2ART.
The SM2ART program focuses on developing an infrastructure-scale factory of the future, where sustainable, carbon-storing biomaterials are used to build everything from houses, ships and automobiles to clean energy infrastructure such as wind turbine components, Ozcan said.
“Creating strong, affordable, carbon-neutral materials for 3D printers gives us an edge to solve issues like the housing shortage,” Smith said.
It typically takes about six months to build a house using conventional methods. But with the right mix of materials and additive manufacturing, producing and assembling sustainable, modular housing components could take just a day or two, the scientists added.
The team continues to pursue additional pathways for more cost-effective nanocellulose production, including new drying processes. Follow-on research is expected to use simulations to also predict the best combination of nanocellulose and other polymers to create fiber-reinforced composites for advanced manufacturing systems such as the ones being developed and refined at DOE’s Manufacturing Demonstration Facility, or MDF, at ORNL. The MDF, supported by AMMTO, is a nationwide consortium of collaborators working with ORNL to innovate, inspire and catalyze the transformation of U.S. manufacturing.
For more information: PNAS
Image: ORNL scientists used molecular dynamics simulations, exascale computing, lab testing and analysis to accelerate the development of an energy-saving method to produce nanocellulosic fibers. This strong, lightweight, material is ideal for 3D-printing of sustainable housing, vehicles and clean energy components.
Solar energy breakthrough could reduce need for solar farms
Scientists at Oxford University have developed a groundbreaking approach to generating solar electricity without silicon-based panels. Their innovation involves coating a new, ultra-thin, and flexible light-absorbing material onto everyday objects like rucksacks, cars, and mobile phones. This material uses a multi-junction technique to stack multiple light-absorbing layers into one solar cell, capturing a broader spectrum of light and generating more power from the same amount of sunlight.
This new material has been independently certified to achieve over 27% energy efficiency, matching the performance of traditional silicon photovoltaics for the first time. The certification from Japan’s National Institute of Advanced Industrial Science and Technology (AIST) precedes the publication of the researchers’ study later this year.
“During just five years experimenting with our stacking or multi-junction approach, we have raised power conversion efficiency from around 6% to over 27%, close to the limits of what single-layer photovoltaics can achieve today,” said Dr Shuaifeng Hu, Post Doctoral Fellow at Oxford University Physics. “We believe that, over time, this approach could enable the photovoltaic devices to achieve far greater efficiencies, exceeding 45%.”
This compares with around 22% energy efficiency from solar panels today (meaning they convert around 22% of the energy in sunlight), but the versatility of the new ultra-thin and flexible material is also key. At just over one micron thick, it is almost 150 times thinner than a silicon wafer. Unlike existing photovoltaics, generally applied to silicon panels, this can be applied to almost any surface.
‘By using new materials that can be applied as a coating, we’ve shown we can replicate and out-perform silicon while also gaining flexibility. This is important because it promises more solar power without the need for so many silicon-based panels or specially built solar farms,’ said Dr Junke Wang, Marie Skłodowska Curie Actions Postdoc Fellow at Oxford University Physics.
The researchers believe their approach will continue to reduce solar costs and make it the most sustainable form of renewable energy. Since 2010, the global average cost of solar electricity has fallen by almost 90%, making it almost a third cheaper than that generated from fossil fuels. Innovations promise additional cost savings as new materials, like thin-film perovskite, reduce the need for silicon panels and purpose-built solar farms.
The researchers are among 40 scientists working on photovoltaics led by Professor of Renewable Energy Henry Snaith at Oxford University Physics Department. Their pioneering work in photovoltaics and especially the use of thin-film perovskite began around a decade ago and benefits from a bespoke, robotic laboratory.
Their work has strong commercial potential and has already started to feed through into applications across the utilities, construction, and car manufacturing industries.
For more information: University of Oxford
Image: Dr Shuaifeng Hu, Post Doctoral Fellow at Oxford University Physics, examining the new thin-film perovskite material. Image credit: Martin Small.
Revolutionary gel could save homes from devastating wildfires
As climate change leads to hotter and drier conditions, fire seasons are becoming longer and wildfires more frequent and severe, devastating communities and economies. To address this growing threat, Stanford researchers have developed a water-enhancing gel that can be sprayed on homes and critical infrastructure to prevent them from burning during wildfires. This new gel lasts longer and is significantly more effective than existing commercial gels, providing extended protection even when applied well in advance of a fire, according to Eric Appel, associate professor of materials science and engineering.
Water-enhancing gels are made of super-absorbent polymers – similar to the absorbent powder found in disposable diapers. Mixed with water and sprayed on a building, they swell into a gelatinous substance that clings to the outside of the structure, creating a thick, wet shield. But the conditions near a wildfire are extremely dry – temperatures can be near 100 degrees, with high winds and zero percent humidity – and even water locked in a gel evaporates fairly quickly.
In the gel Appel and his colleagues designed, the water is just the first layer of protection. In addition to a cellulose-based polymer, the gel contains silica particles, which get left behind when the gels are subjected to heat.
“We have discovered a unique phenomenon where a soft, squishy hydrogel seamlessly transitions into a robust aerogel shield under heat, offering enhanced and long-lasting wildfire protection. This environmentally conscious breakthrough surpasses current commercial solutions, offering a superior and scalable defense against wildfires,” said the study’s lead author, Changxin “Lyla” Dong.
“When the water boils off, and all of the cellulose burns off, we’re left with the silica particles assembled into a foam,” Appel said. “That foam is highly insulative and ends up scattering all of the heat, completely protecting the substrate underneath it.”
The silica forms an aerogel – a solid, porous structure that is a particularly good insulator. Similar silica aerogels are used in space applications because they are extremely lightweight and can prevent most methods of heat transfer.
The researchers tested several formulations of their new gel by applying them to pieces of plywood and exposing them to direct flame from a gas hand torch, which burns at a considerably higher temperature than wildfire. Their most effective formulation lasted for more than 7 minutes before the board began to char. When they tested a commercially available water-enhancing gel in the same way, it protected the plywood for less than 90 seconds.
“Traditional gels don’t work once they dry out,” Appel said. “Our materials form this silica aerogel when exposed to fire that continues to protect the treated substrates after all the water has evaporated. These materials can be easily washed away once the fire is gone.”
The new gels build off of Appel’s previous wildfire prevention work. In 2019, Appel and his colleagues used these same gels as a vehicle to hold wildland fire retardants on vegetation for months at a time. The formulation was intended to help prevent ignition in wildfire-prone areas.
“We’ve been working with this platform for years now,” Appel said. “This new development was somewhat serendipitous – we were wondering how these gels would behave on their own, so we just smushed some on a piece of wood and exposed it to flames from a torch we had lying around the lab. What we observed was this super cool outcome where the gels puffed up into an aerogel foam.”
After that initial success, several years of additional engineering were needed to optimize the formulation. It is now stable in storage, easily sprayable with standard equipment, and adheres well to all kinds of surfaces. The gels are made of nontoxic components that have already been approved for use by the U.S. Forest Service, and the researchers conducted studies to show that they are easily broken down by soil microbes.
“They’re safe for both people and the environment,” Appel said. “There may need to be additional optimization, but my hope is that we can do pilot-scale application and evaluation of these gels so we can use them to help protect critical infrastructure when a fire comes through.”
For more information: Advanced Materials
Image: During a test on plywood, researchers showed how the new gel transitions from a hydrogel to an aerogel under heat from a gas hand torch. The torch burned at a much higher temperature than would result from a wildfire. Credit: Andrea d’Aquino
Unconventional interface superconductor could benefit quantum computing
A team of scientists, led by physicist Peng Wei at the University of California, Riverside, has developed a new superconductor material with potential applications in quantum computing. This material could be a candidate for a “topological superconductor,” which uses a delocalized state of an electron or hole to robustly carry quantum information and process data.
The researchers combined trigonal tellurium, a chiral and non-magnetic material, with a surface-state superconductor on a thin film of gold. They observed quantum states at the interface with well-defined spin polarization, which could be used to create spin quantum bits (qubits). This breakthrough could significantly advance the field of quantum computing.
“By creating a very clean interface between the chiral material and gold, we developed a two-dimensional interface superconductor,” said Wei, an associate professor of physics and astronomy. “The interface superconductor is unique as it lives in an environment where the energy of the spin is six times more enhanced than those in conventional superconductors.”
The researchers observed that the interface superconductor undergoes a transition under a magnetic field and becomes more robust at a high field compared with the low field, which suggests a transition into a “triplet superconductor,” which is more stable under a magnetic field.
Furthermore, through collaboration with scientists at the National Institute of Standards and Technology, the researchers showed that such a superconductor involving heterostructure gold and niobium thin films naturally suppresses decoherence sources from material defects such as niobium oxides that are a common challenge for niobium superconductors. They showed that the superconductor can be made into high-quality low-loss microwave resonators with a quality factor reaching 1 million.
According to the multinational technology company IBM, the new technology has applications in quantum computing, a field that uses quantum mechanics to solve complex problems that classical computers or supercomputers cannot solve or cannot solve quickly enough.
“We achieved this using materials that are one order of magnitude thinner than those typically used in the quantum computing industry,” Wei said. “The low-loss microwave resonators are critical components of quantum computing and could lead to low-loss superconducting qubits. The biggest challenge in quantum computing is to reduce decoherence or quantum information loss in a qubit system.”
Decoherence occurs when a quantum system interacts with its environment, causing the system’s information to get mixed up with the environment. Decoherence poses a challenge for realizing quantum computers.
Unlike previous methods that require magnetic materials, the researchers’ new approach uses non-magnetic materials for a cleaner interface.
“Our material could be a promising candidate for developing more scalable and reliable quantum computing components,” Wei said.
For more information: Science Advances
Image: Peng Wei
Oxford Instruments completed acquisition of FemtoTools AG
Oxford Instruments plc, United Kingdom, a leading provider of high technology products and services to industry and scientific research communities, completed the acquisition of FemtoTools AG, Switzerland. The acquisition was first announced on 11 June 2024, and has been completed following the satisfactory conclusion of closing conditions.
FemtoTools specializes in measuring and imaging the properties (primarily the hardness and stiffness) of materials for research and semiconductor applications at very high resolution via a technique called nanoindentation. It joins Oxford Instruments’ Imaging & Analysis division, where its products will be sold in conjunction with the Group’s existing range of materials analysis tools, including electron microscope micro-analyzers and Raman microscopes.
Richard Tyson, chief executive officer, Oxford Instruments plc, said: “We are delighted to have completed the acquisition of FemtoTools. We welcome our new colleagues and look forward to working with them to integrate nanoindentation – a new technique to Oxford Instruments – into our extensive portfolio of materials analysis capabilities.”
Christian Lang, managing director, Materials Analysis, Oxford Instruments plc, said: “We’re so pleased that the FemtoTools team have chosen to join Oxford Instruments. We’ve had a number of very positive meetings since the announcement and are already making plans for our future together.
“I’m looking forward to integrating FemtoTools’ brilliant technology into our wider product range, and to working with this talented group of people.”
Felix Beyeler, co-founder of FemtoTools, said: “The team and I are very excited for the journey ahead as part of Oxford Instruments. Working together will enable us to extend the reach of our technology and provide even richer analysis to our combined customer base. We’re also looking forward to learning from the hugely experienced Oxford Instruments team.”
For more information:
Oxford Instruments plc
https://www.oxinst.com
Kyocera introduces cutting-edge Peltier module with 21% increase in cooling performance
Kyocera Corporation, Japan, launched a new Peltier (thermoelectric) module that boasts a maximum heat absorption rate 21% higher than its conventional products, significantly enhancing cooling performance for applications such as automotive battery and seat temperature control.
Continue readingArtificial intelligence helped scientists create a new type of battery
Researchers at Microsoft, Redmond, Wash., and Pacific Northwest National Laboratory, Richland, Wash., used artificial intelligence to identify 23 promising battery materials from more than 32 million candidates in just 80 hours, creating a working prototype that could significantly reduce lithium use and advance sustainable energy storage solutions.
Continue readingSuper-black wood can improve telescopes, optical devices and consumer goods
Researchers at the University of British Columbia, led by Professor Philip Evans and PhD student Kenny Cheng, accidentally discovered a super-black material that absorbs almost all light, potentially useful in fine jewelry, solar cells, and precision optical devices. While experimenting with high-energy plasma to make wood more water-repellent, they found that applying the technique to the cut ends of wood cells turned the surfaces extremely black. Measurements by Texas A&M University’s Department of Physics and Astronomy confirmed that this material reflects less than one percent of visible light, absorbing nearly all the light that strikes it.
Instead of discarding this accidental finding, the team shifted their focus to designing super-black materials, contributing a new approach to the search for the darkest materials on Earth.
“Ultra-black or super-black material can absorb more than 99 percent of the light that strikes it – significantly more so than normal black paint, which absorbs about 97.5 percent of light,” explained Dr. Evans, a professor in the faculty of forestry and BC Leadership Chair in Advanced Forest Products Manufacturing Technology.
Super-black materials are increasingly sought after in astronomy, where ultra-black coatings on devices help reduce stray light and improve image clarity. Super-black coatings can enhance the efficiency of solar cells. They are also used in making art pieces and luxury consumer items like watches.
The researchers have developed prototype commercial products using their super-black wood. They initially focused on watches and jewelry but plan to explore other commercial applications in the future.
The team named and trademarked their discovery Nxylon (niks-uh-lon), after Nyx, the Greek goddess of the night, and xylon, the Greek word for wood.
Most surprisingly, Nxylon remains black even when coated with an alloy, such as the gold coating applied to the wood to make it electrically conductive enough to be viewed and studied using an electron microscope. This is because Nxylon’s structure inherently prevents light from escaping rather than depending on black pigments.
The UBC team have demonstrated that Nxylon can replace expensive and rare black woods like ebony and rosewood for watch faces, and it can be used in jewelry to replace the black gemstone onyx.
“Nxylon’s composition combines the benefits of natural materials with unique structural features, making it lightweight, stiff and easy to cut into intricate shapes,” said Dr. Evans.
Made from basswood, a tree widely found in North America and valued for hand carving, boxes, shutters and musical instruments, Nxylon can also use other types of wood such as European lime wood.
Dr. Evans and his colleagues plan to launch a startup, Nxylon Corporation of Canada, to scale up applications of Nxylon in collaboration with jewellers, artists and tech product designers. They also plan to develop a commercial-scale plasma reactor to produce larger super-black wood samples suitable for non-reflective ceiling and wall tiles.
“Nxylon can be made from sustainable and renewable materials widely found in North America and Europe, leading to new applications for wood. The wood industry in B.C. is often seen as a sunset industry focused on commodity products—our research demonstrates its great untapped potential,” said Dr. Evans.
For more information: The University of British Columbia
Image: UBC forestry researchers have created a new super-black material that absorbs almost all light. From left, Dengcheng Feng, Kenny Cheng, Dr. Philip Evans and Sara Xu. Credit: UBC Forestry/Ally Penders